Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Pure/Low Nickel Alloy
DIN 17740 Grade LC-Ni99 soft annealed (+A)Pure/Low Nickel Alloy
DIN 17740 Grade Ni99.2 soft annealed (+A)Nitriding Steel
EN 10085 Grade 31CrMoV9 quenched and tempered (+QT)Malleable Cast Iron
EN 1562 Grade GJMW-360-12 decarburized annealedMalleable Cast Iron
EN 1562 Grade GJMW-400-5 decarburized annealedMalleable Cast Iron
EN 1562 Grade GJMW-450-7 decarburized annealedNitriding Steel
EN 10085 Grade 31CrMo12 quenched and tempered (+QT)Malleable Cast Iron
EN 1562 Grade GJMW-350-4 decarburized annealedHierro fundido
EN 1562 Grade GJMB-350-10 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-450-6 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-550-4 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-650-2 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-700-2 not decarburized annealed