Elongación: 105 %

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-20

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 460

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2821-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2801-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-07

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-04

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2751-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 PC

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 WR

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2900-04

Suministrada por:

Arkema: High Performance Polymers

Policarbonato (PC)

LEXAN™ Resin LUX2110T

6000 Serie

AA Standards Grade 6063 T1

Suministrada por:

2 proveedores de Matmatch

6000 Serie

AA Standards Grade 6063 T5

Suministrada por:

2 proveedores de Matmatch

6000 Serie

AA Standards Grade 6063 T6

Suministrada por:

2 proveedores de Matmatch

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850 Black

Suministrada por:

Arkema: High Performance Polymers

Copoliéster termoplástico

Arnitel® ECO M700

Suministrada por:

DSM Engineering Materials

Polipropileno

Polypropylene Homopolymer (PPH)

Suministrada por:

1 proveedor Matmatch

Polipropileno

Polypropylene Random Copolymer (PPR)

Suministrada por:

1 proveedor Matmatch

Página 1 de 3