Elongation at yield: 27 %

Quick Comparison

Copoliéster termoplástico

Hytrel® 6359FG NC010

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3030-10

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3030-15

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3030-50

Suministrada por:

Arkema: High Performance Polymers

Polioximetileno (POM)

Delrin® 100T BK602

Copoliéster termoplástico

Arnitel® JD7515

Suministrada por:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar Flex® Ultraflex B

Suministrada por:

Arkema: High Performance Polymers