General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.26 g/cm³ Show Supplier Material materials with Density of 1.26 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Water absorption | 0.6 % Show Supplier Material materials with Water absorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 0.36 GPa Show Supplier Material materials with Elastic modulus of 0.36 GPa | dry | ISO 527-1/-2 | ||
Elongation | 50 % Show Supplier Material materials with Elongation of 50 % | dry | ISO 527-1/-2 | ||
300 % Show Supplier Material materials with Elongation of 300 % | dry | ISO 527-1/-2 | |||
Hardness, Shore D | 71 [-] Show Supplier Material materials with Hardness, Shore D of 71 [-] | dry | ISO 868 | 3s | |
Impact strength, Charpy notched | 23 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | dry | ISO 179/1eA | |
Tensile strength | 30.8 MPa Show Supplier Material materials with Tensile strength of 30.8 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.75e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.75e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.75e-06 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.75e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 52 °C Show Supplier Material materials with Heat deflection temperature of 52 °C | dry | ISO 75-1/-2 | 2 MPa | |
Melting point | 216 °C Show Supplier Material materials with Melting point of 216 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt mass-flow rate | 230 °C | 28.0 g/10min Show Supplier Material materials with Melt mass-flow rate of 28.0 g/10min | dry | ISO 1133 | |
Shrinkage | 1.75 % Show Supplier Material materials with Shrinkage of 1.75 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Shrinkage of 2 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property |
---|