Heat deflection temperature, 1.80 MPa: 215 °C

Quick Comparison

Polieterimida (PEI)

ULTEM™ Resin HU1000 - Europe

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1000 - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin HU1000 - Americas

Suministrada por:

Sabic

Other Polyamide (PA)

Zytel® HTNFR55G50NHLW BK046

Polyamide 410 (PA410)

EcoPaXX® Q-HG6

Suministrada por:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q-KG6-FC

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

EPLAMID 6 GFS 60 HS BK Q2G001 (PA6)

Suministrada por:

EPSAN

Polyamide 66 (PA66)

EPLAMID 66 GFS 30 HS NC Q1D004 (PA66)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFU 30 UVL NC Q2D001 (PA6)

Suministrada por:

EPSAN

Polyamide 410 (PA410)

EcoPaXX® Q-KG6

Suministrada por:

DSM Engineering Materials

Polieterimida (PEI)

ULTEM™ Resin CRS5111 - Asia

Suministrada por:

Sabic

Polieterimida (PEI)

ULTEM™ Resin CRS5111 - Americas

Suministrada por:

Sabic

Polyamide 66 (PA66)

TECACOMP PA66 ID blue 1050909

Suministrada por:

Ensinger GmbH

Polyamide 6 (PA6)

Zytel® 73G40T BK416

Polyamide 410 (PA410)

EcoPaXX® Q-HG10

Suministrada por:

DSM Engineering Materials

Polietileno tereftalato (PET)

VYPET™ VNT-325

Suministrada por:

Lavergne

Polieterimida (PEI)

ULTEM™ Resin CRS5311 - Europe

Suministrada por:

Sabic

Polyamide 6 (PA6)

PA6 B2730G

Suministrada por:

HENAN SHENMA HUAWEI PLASTIC CO.,LTD.

Polyamide 6 (PA6)

LNP™ THERMOCOMP™ Compound PF007 - Europe

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ THERMOCOMP™ Compound WF008 - Asia

Suministrada por:

Sabic
Página 1 de 2