General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Density | 1.52 g/cm³ Show Supplier Material materials with Density of 1.52 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 12 GPa Show Supplier Material materials with Elastic modulus of 12 GPa | conditioned | ISO 527-1/-2 | |
16 GPa Show Supplier Material materials with Elastic modulus of 16 GPa | dry | ISO 527-1/-2 | ||
120 °C | 7.6 GPa Show Supplier Material materials with Elastic modulus of 7.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 5.9 GPa Show Supplier Material materials with Elastic modulus of 5.9 GPa | dry | ISO 527-1/-2 | |
180 °C | 4.9 GPa Show Supplier Material materials with Elastic modulus of 4.9 GPa | dry | ISO 527-1/-2 | |
200 °C | 3.9 GPa Show Supplier Material materials with Elastic modulus of 3.9 GPa | dry | ISO 527-1/-2 | |
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-1/-2 | |
3.5 % Show Supplier Material materials with Elongation of 3.5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 6.4 % Show Supplier Material materials with Elongation of 6.4 % | dry | ISO 527-1/-2 | |
160 °C | 7.7 % Show Supplier Material materials with Elongation of 7.7 % | dry | ISO 527-1/-2 | |
180 °C | 8.4 % Show Supplier Material materials with Elongation of 8.4 % | dry | ISO 527-1/-2 | |
200 °C | 9.8 % Show Supplier Material materials with Elongation of 9.8 % | dry | ISO 527-1/-2 | |
Flexural modulus | 11.3 GPa Show Supplier Material materials with Flexural modulus of 11.3 GPa | conditioned | ISO 178 | |
14.6 GPa Show Supplier Material materials with Flexural modulus of 14.6 GPa | dry | ISO 178 | ||
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |
335 MPa Show Supplier Material materials with Flexural yield strength of 335 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | -30 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA |
23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 19 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 19 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m² | dry | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 85 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 170 MPa Show Supplier Material materials with Tensile strength of 170 MPa | conditioned | ISO 527-1/-2 | |
220 MPa Show Supplier Material materials with Tensile strength of 220 MPa | dry | ISO 527-1/-2 | ||
120 °C | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | dry | ISO 527-1/-2 | |
160 °C | 95 MPa Show Supplier Material materials with Tensile strength of 95 MPa | dry | ISO 527-1/-2 | |
180 °C | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | dry | ISO 527-1/-2 | |
200 °C | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 4.2e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Heat deflection temperature | 215 °C Show Supplier Material materials with Heat deflection temperature of 215 °C | dry | ISO 75-1/-2 | 2 MPa | |
245 °C Show Supplier Material materials with Heat deflection temperature of 245 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 250 °C Show Supplier Material materials with Melting point of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Charge Air Cooler Caps, Crankshaft Covers | |
Fillers | 50% Glass Fiber |