EPLAMID 6 GFS 60 HS BK Q2G001 (PA6)

Alternative and trade names
PA6-GF60
Want to keep this datasheet? Save it now in your required format

Description

Polyamide 6, reinforced with 60% of glass fiber, heat aging stabilized, lubricated for injection moulding with improved mechanical properties.

Eplamid 6 glass fiber reinforced compounds are used in all sectors of industry, offering a good balance of thermal and mechanical properties.

This material data has been provided by Epsan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.69 g/cm³

Show Supplier Material materials with Density of 1.69 g/cm³

ISO 1183

Water content

23.0 °C

0.1 %

Show Supplier Material materials with Water content of 0.1 %

ISO 15512

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

20 GPa

Show Supplier Material materials with Elastic modulus of 20 GPa

ISO 527-2 (1mm/min)

Elongation

23.0 °C

2.5 %

Show Supplier Material materials with Elongation of 2.5 %

ISO 527-2 (5mm/min)

Flexural modulus

23.0 °C

18 GPa

Show Supplier Material materials with Flexural modulus of 18 GPa

ISO 178 (2mm/min)

Flexural strength

23.0 °C

320 MPa

Show Supplier Material materials with Flexural strength of 320 MPa

ISO 178 (2mm/min)

Impact strength, Charpy notched

23.0 °C

16 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

95 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m²

ISO 179/1eU

Impact strength, Izod notched

23.0 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m²

ISO 180/1A

Impact strength, Izod unnotched

23.0 °C

90 kJ/m²

Show Supplier Material materials with Impact strength, Izod unnotched of 90 kJ/m²

ISO 180/1U

Tensile strength

23.0 °C

220 MPa

Show Supplier Material materials with Tensile strength of 220 MPa

ISO 527-2 (5mm/min)

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

60 %

Show Supplier Material materials with Ash content of 60 %

ISO 3451-4

Heat deflection temperature, 0.45 MPa

220 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C

ISO 75-2/B

Heat deflection temperature, 1.80 MPa

215 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 215 °C

ISO 75-2/A

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ISO 3146

Flammability

UL94 (0.8mm) HB, EN 60695-11-10

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

500 V

Show Supplier Material materials with Comparative tracking index of 500 V

EN 60112

Surface resistivity

23.0 °C

1.00E+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

ISO 294-4 (3mm)

Shrinkage, transverse

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage, transverse of 0.3 %

ISO 294-4 (3mm)

Technological properties

Property
Application areas

Eplamid 6 glass fiber reinforced compounds are used in all sectors of industry, offering a good balance of thermal and mechanical properties. Eplamid 6 is suitable for applications in direct contact with drinking water and food.

Certifications

Drinking Water,Food Contact

Fillers

60% Glass Fiber

Other

Laboratory conditions are 23 ±2°C and 45-55 % RH.