TECACOMP PA66 ID blue 1050909

Alternative and trade names
PA66-MD
Want to keep this datasheet? Save it now in your required format

Description

PA 66 (Polyamide 66) filled with Detectable filler. Main features: detectable via metal detector, x-ray detectable, Explanation of food contact according to FDA and EU 10/2011 on request, Heat Stabilized and UV Stabilized

This material data has been provided by Ensinger GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

1.39 g/cm³

Show Supplier Material materials with Density of 1.39 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.5 GPa

Show Supplier Material materials with Elastic modulus of 2.5 GPa

DIN EN ISO 527-1

Elongation

23.0 °C

16 %

Show Supplier Material materials with Elongation of 16 %

DIN EN ISO 527-1

Impact strength, Charpy unnotched

23.0 °C

87 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 87 kJ/m²

DIN EN ISO 179-1eU

Tensile strength

23.0 °C

54 MPa

Show Supplier Material materials with Tensile strength of 54 MPa

DIN EN ISO 527-1

Thermal

PropertyValueComment

Glass transition temperature

72 °C

Show Supplier Material materials with Glass transition temperature of 72 °C

Heat deflection temperature, 1.80 MPa

215 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 215 °C

ISO-R 75 Method A

Max service temperature, long

110 °C

Show Supplier Material materials with Max service temperature, long of 110 °C

Max service temperature, short

170 °C

Show Supplier Material materials with Max service temperature, short of 170 °C

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

Flammability

UL94 class HB for 0.8mm thickness, DIN IEC 60695-11-10

Rheological Properties

PropertyValueComment

Melt mass-flow rate

28 g/10min

Show Supplier Material materials with Melt mass-flow rate of 28 g/10min

DIN EN ISO 1133, 280°C/2.16kg

Technological properties

Property
Certifications

Explanation of food contact according to FDA and EU 10/2011 on request

Color

Blue

Detectability

Inductive: 4.7 mm Al

Fillers

Detectable Filler

Processing methods

Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 8, mould temperature (°C): 150, material temperature (°C): 310, cylinder/processing temperature (°C): 310