Resistencia al choque, ensayo Charpy entallado: 5 kJ/m²

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 720

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 720 RED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 740

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 740 RED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 720 MED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 710

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2850-00

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2800-20

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 9000 HD

Suministrada por:

Arkema: High Performance Polymers

Tereftalato de polibutileno (PBT)

LNP™ THERMOCOMP™ Compound WF006XXP

Suministrada por:

Sabic

Polyvinylidenefluoride (PVDF)

Kynar® 1000 HD

Suministrada por:

Arkema: High Performance Polymers

Tereftalato de polibutileno (PBT)

Crastin® S600F20 NC010

Éter de polifenileno (PPE)

NORYL™ Resin V0150B - Europe

Suministrada por:

Sabic

Polyamide 6 (PA6)

Akulon® F223-D

Suministrada por:

DSM Engineering Materials

Copoliéster termoplástico

Hytrel® 8238

Mezcla de polímeros

VALOX™ FR Resin ENH8530 - Europe

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

VALOX™ FR Resins DR48

Polyamide 6 (PA6)

Akulon® K222-D

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K225-KS

Suministrada por:

DSM Engineering Materials
Página 1 de 13