General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.54 g/cm³ Show Supplier Material materials with Density of 1.54 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 9.2 GPa Show Supplier Material materials with Elastic modulus of 9.2 GPa | dry | ISO 527-1/-2 | |
Elongation | 2.1 % Show Supplier Material materials with Elongation of 2.1 % | dry | ISO 527-1/-2 | |
Flexural modulus | 6 GPa Show Supplier Material materials with Flexural modulus of 6 GPa | conditioned | ISO 178 | |
7.7 GPa Show Supplier Material materials with Flexural modulus of 7.7 GPa | dry | ISO 178 | ||
Flexural yield strength | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | conditioned | ISO 178 | |
205 MPa Show Supplier Material materials with Flexural yield strength of 205 MPa | dry | ISO 178 | ||
Impact strength, Charpy notched | 23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | conditioned | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 38 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 38 kJ/m² | dry | ISO 179/1eU |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 55.0 kJ/m² | conditioned | ISO 179/1eU | |
Tensile strength | 135 MPa Show Supplier Material materials with Tensile strength of 135 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Thickness | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 3e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Heat deflection temperature of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 225 V Show Supplier Material materials with Comparative tracking index of 225 V | dry | IEC 60112 | |
Dielectric constant | 4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
Dielectric strength | 23 kV/mm Show Supplier Material materials with Dielectric strength of 23 kV/mm | dry | IEC 60243-1 | |
Dissipation factor | 200 [-] Show Supplier Material materials with Dissipation factor of 200 [-] | dry | IEC 62631-2-1 | 1MHz |
Surface resistivity | 8e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 8e+12 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 8e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 8e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |