SAE J775 Grade EV-16 For Mechanical Tests: ST+P

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

205 GPa

Show Material materials with Elastic modulus of 205 GPa

Elongation A5

23.0 °C

20 %

Show Material materials with Elongation A5 of 20 %

Hardness, Rockwell C

23.0 °C

25 [-]

Show Material materials with Hardness, Rockwell C of 25 [-]

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Austenitic Stainless Steel

Reduction of area

23.0 °C

30 - 33 %

Show Material materials with Reduction of area of 30 - 33 %

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Austenitic Stainless Steel

Tensile strength

23.0 °C

850 - 1100 MPa

Show Material materials with Tensile strength of 850 - 1100 MPa

Yield strength

23.0 °C

550 - 634 MPa

Show Material materials with Yield strength of 550 - 634 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.65E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.65E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

300.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

500.0 °C

1.73E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.73E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

700.0 °C

1.74E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.74E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

Melting point

1230 - 1480 °C

Show Material materials with Melting point of 1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

23.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

23.0 °C

14.5 W/(m·K)

Show Material materials with Thermal conductivity of 14.5 W/(m·K)

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

8.5E-7 Ω·m

Show Material materials with Electrical resistivity of 8.5E-7 Ω·m

Typical for Austenitic Stainless Steel

Chemical properties

PropertyValue

Carbon

0.28 - 0.38 %

Show Material materials with Carbon of 0.28 - 0.38 %

Chromium

22 - 24 %

Show Material materials with Chromium of 22 - 24 %

Iron

64.59 - 100 %

Show Material materials with Iron of 64.59 - 100 %

Manganese

1.5 - 3.5 %

Show Material materials with Manganese of 1.5 - 3.5 %

Molybdenum

0.5 %

Show Material materials with Molybdenum of 0.5 %

Nickel

7 - 9 %

Show Material materials with Nickel of 7 - 9 %

Nitrogen

0.25 - 0.35 %

Show Material materials with Nitrogen of 0.25 - 0.35 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

0.5 - 1 %

Show Material materials with Silicon of 0.5 - 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

0.5 %

Show Material materials with Tungsten of 0.5 %