Acero bajo en carbono
EN 10028-3 Grade P275NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10028-3 Grade P275NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10028-3 Grade P355NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10028-3 Grade P355NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Nickel Steel
EN 10028-4 Grade X12Ni5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Nickel Steel
EN 10028-4 Grade 11MnNi5-3 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Nickel Steel
EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Nickel Steel
EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P500QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P690QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P355ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch