Acero inoxidable ferrítico
DIN 17440 Grade X6CrAl13 soft annealed (+A)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Acero inoxidable martensítico
EN 10088-1 Grade X6Cr13 soft annealed (+A)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Acero inoxidable austenítico
EN 10028-7 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Acero inoxidable ferrítico
EN 10088-1 Grade X6CrAl13 soft annealed (+A)Nickel Chromium Alloy
DIN 17742 Grade NiCr15Fe soft annealed (+A)Acero inoxidable martensítico
DIN 17440 Grade X6Cr13 soft annealed (+A)Acero bajo en carbono
DIN 17245 Grade GS-C25 normalized or normalized formed (+N)Acero inoxidable ferrítico
EN 10095 Grade X10CrAlSi7 soft annealed (+A)Acero inoxidable austenítico
EN 10095 Grade X15CrNiSi25-4 solution annealed (+AT)Acero inoxidable ferrítico
SEW 470 Grade X10CrAlSi7 soft annealed (+A)Acero bajo en carbono
EN 10213 Grade GP240GH normalized or normalized formed (+N)Acero bajo en carbono
EN 10213 Grade GP240GH quenched and tempered (+QT)Acero bajo en carbono
DIN 5512-2 Grade St 37-2 G cold rolledAcero inoxidable martensítico
DIN 17243 Grade X20CrMoV12-1 quenched and tempered (+QT)