Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.85 g/cm³ Show Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 211 GPa Show Material materials with Elastic modulus of 211 GPa | |
100.0 °C | 204 GPa Show Material materials with Elastic modulus of 204 GPa | ||
200.0 °C | 196 GPa Show Material materials with Elastic modulus of 196 GPa | ||
300.0 °C | 186 GPa Show Material materials with Elastic modulus of 186 GPa | ||
400.0 °C | 177 GPa Show Material materials with Elastic modulus of 177 GPa | ||
500.0 °C | 164 GPa Show Material materials with Elastic modulus of 164 GPa | ||
600.0 °C | 127 GPa Show Material materials with Elastic modulus of 127 GPa | ||
Elongation | 20.0 °C | 22 % Show Material materials with Elongation of 22 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Low Carbon Steel |
Shear modulus | 23.0 °C | 82 GPa Show Material materials with Shear modulus of 82 GPa | Typical for Low Carbon Steel |
Tensile strength | 20.0 °C | 440 - 590 MPa Show Material materials with Tensile strength of 440 - 590 MPa | |
Yield strength | 20.0 °C | 245 MPa Show Material materials with Yield strength of 245 MPa | |
Yield strength Rp0.2 | 200.0 °C | 175 MPa Show Material materials with Yield strength Rp0.2 of 175 MPa | |
300.0 °C | 145 MPa Show Material materials with Yield strength Rp0.2 of 145 MPa | ||
350.0 °C | 135 MPa Show Material materials with Yield strength Rp0.2 of 135 MPa | ||
400.0 °C | 130 MPa Show Material materials with Yield strength Rp0.2 of 130 MPa | ||
450.0 °C | 125 MPa Show Material materials with Yield strength Rp0.2 of 125 MPa | ||
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.22E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.22E-5 1/K | |
200.0 °C | 1.29E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.29E-5 1/K | ||
300.0 °C | 1.34E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.34E-5 1/K | ||
400.0 °C | 1.39E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K | ||
500.0 °C | 1.43E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.43E-5 1/K | ||
600.0 °C | 1.46E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.46E-5 1/K | ||
Max service temperature | 500 °C Show Material materials with Max service temperature of 500 °C | Typical for Carbon Steel | |
Max service temperature, long | 300 - 610 °C Show Material materials with Max service temperature, long of 300 - 610 °C | ||
Melting point | 1480 - 1526 °C Show Material materials with Melting point of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Specific heat capacity | 20.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 50 W/(m·K) Show Material materials with Thermal conductivity of 50 W/(m·K) | |
300.0 °C | 46 W/(m·K) Show Material materials with Thermal conductivity of 46 W/(m·K) | ||
400.0 °C | 42 W/(m·K) Show Material materials with Thermal conductivity of 42 W/(m·K) | ||
500.0 °C | 38 W/(m·K) Show Material materials with Thermal conductivity of 38 W/(m·K) | ||
600.0 °C | 34 W/(m·K) Show Material materials with Thermal conductivity of 34 W/(m·K) | ||
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 1.6E-7 Ω·m Show Material materials with Electrical resistivity of 1.6E-7 Ω·m |
Magnetic
Property | Value | Comment |
---|---|---|
Curie temperature | 770 °C Show Material materials with Curie temperature of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Carbon | 0.18 - 0.23 % Show Material materials with Carbon of 0.18 - 0.23 % |
Chromium | 0.3 % Show Material materials with Chromium of 0.3 % |
Manganese | 0.5 - 0.8 % Show Material materials with Manganese of 0.5 - 0.8 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.3 - 0.6 % Show Material materials with Silicon of 0.3 - 0.6 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |