Acero inoxidable austenítico
Esshete 1250Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2507® Solution AnnealedSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2507® Cold WorkedSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
Sandvik 5R10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
Sandvik 3R12Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
Sandvik 6R35Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2906™Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiN18-10 solution annealed (+AT)Acero inoxidable austenítico
1.4571 / X6CrNiMoTi17-2-2Suministrada por:
HSM Stahl- und Metallhandel GmbH