Specific Electrical conductivity: 32 % IACS

Quick Comparison

Bronce fosforado

HRD200 Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper Bronze Silicon Bronze

EN 1652 Grade CuNi2Si TH