General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 13.7 g/cm³ Show Material materials with Density of 13.7 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Flexural strength | 20.0 °C | 896 - 965 MPa Show Material materials with Flexural strength of 896 - 965 MPa |
Hardness, Rockwell B | 20.0 °C | 85 - 98 [-] Show Material materials with Hardness, Rockwell B of 85 - 98 [-] |
Tensile strength | 20.0 °C | 516 - 585 MPa Show Material materials with Tensile strength of 516 - 585 MPa |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 29 - 52 % IACS Show Material materials with Specific Electrical conductivity of 29 - 52 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | 28 - 32 % Show Material materials with Copper of 28 - 32 % |