See where Pink Sheets Grade 201.0 T7 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ3.1 g/cm³ at 23 °C
Creep strength
Rm,creepup to 1000 hours
Coefficient of thermal expansion
α2.1E-5 1/K at 23 °C
unstated value between 20°C and the mentioned temperature
Melting point
Tm570 - 649 °C
Specific heat capacity
cp920 J/(kg·K) at 23 °C
Thermal conductivity
λ120 W/(m·K) at 23 °C
Electrical conductivity
σel1.90E+7 S/m at 23 °C
Typical/Derived values
Electrical resistivity
ρel4.35E-8 - 6.25E-8 Ω·m at 23 °C
Typical for Cast 2xx.x Series Aluminium
Specific Electrical conductivity
32 - 34 % IACS
Typical values
Element
Weight %
Comment
92.1 - 95.1 %
4 - 5.2 %
0.4 - 1 %
0.2 - 0.5 %
0.15 - 0.55 %
This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous oys and Special-Purpose Materials,CastAl_Thermal,AluKey.