General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 14.3 g/cm³ Show Material materials with Density of 14.3 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Flexural strength | 20.0 °C | 965 - 1034 MPa Show Material materials with Flexural strength of 965 - 1034 MPa |
Hardness, Rockwell B | 20.0 °C | 89 - 102 [-] Show Material materials with Hardness, Rockwell B of 89 - 102 [-] |
Tensile strength | 20.0 °C | 585 - 654 MPa Show Material materials with Tensile strength of 585 - 654 MPa |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 27 - 48 % IACS Show Material materials with Specific Electrical conductivity of 27 - 48 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | 23 - 27 % Show Material materials with Copper of 23 - 27 % |