Conductividad térmica: 231 W/(m·K)

Quick Comparison

1000 Series

EN 573-3 Grade AW-1350 H111

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade AW-1350 O

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

1000 Series

EN 573-3 Grade AW-1350 H12

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade AW-1350 H18

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade AW-1350 H28

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

1000 Series

EN 573-3 Grade AW-1350 H19

Suministrada por:

1 proveedor Matmatch

1000 Series

EN 573-3 Grade 1050 O

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B9 Grade C17510 TB00
Página 1 de 90