Viscosity number: 145 cm³/gr

Quick Comparison

Polyamide 46 (PA46)

Stanyl® TE250F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6-FC

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW250F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW200F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE250F3

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS200F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS200F6 B-MB

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS200F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE248F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS250F4D

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW271F6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200S6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW271F6J10

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW275F6

Suministrada por:

DSM Engineering Materials
Página 1 de 2