General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.41 g/cm³ Show Supplier Material materials with Density of 1.41 g/cm³ | dry | ISO 1183 |
Limiting oxygen index | 22 % Show Supplier Material materials with Limiting oxygen index of 22 % | dry | ISO 4589-1/-2 |
Moisture absorption | 2.6 % Show Supplier Material materials with Moisture absorption of 2.6 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 6 GPa Show Supplier Material materials with Elastic modulus of 6 GPa | conditioned | ISO 527-1/-2 | |
10 GPa Show Supplier Material materials with Elastic modulus of 10 GPa | dry | ISO 527-1/-2 | ||
120 °C | 5.3 GPa Show Supplier Material materials with Elastic modulus of 5.3 GPa | dry | ISO 527-1/-2 | |
160 °C | 4.8 GPa Show Supplier Material materials with Elastic modulus of 4.8 GPa | dry | ISO 527-1/-2 | |
Elongation | 3.7 % Show Supplier Material materials with Elongation of 3.7 % | dry | ISO 527-1/-2 | |
6 % Show Supplier Material materials with Elongation of 6 % | conditioned | ISO 527-1/-2 | ||
120 °C | 7.5 % Show Supplier Material materials with Elongation of 7.5 % | dry | ISO 527-1/-2 | |
160 °C | 8 % Show Supplier Material materials with Elongation of 8 % | dry | ISO 527-1/-2 | |
Tensile strength | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | conditioned | ISO 527-1/-2 | |
210 MPa Show Supplier Material materials with Tensile strength of 210 MPa | dry | ISO 527-1/-2 | ||
120 °C | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | dry | ISO 527-1/-2 | |
160 °C | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 2.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glass transition temperature | 75 °C Show Supplier Material materials with Glass transition temperature of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Heat deflection temperature | 290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Heat deflection temperature of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 295 °C Show Supplier Material materials with Melting point of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Vicat softening temperature | 290 °C Show Supplier Material materials with Vicat softening temperature of 290 °C | dry | ISO 306 | 50°C/h 50N |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 500 V Show Supplier Material materials with Comparative tracking index of 500 V | dry | IEC 60112 | |
Dielectric constant | 3.6 [-] Show Supplier Material materials with Dielectric constant of 3.6 [-] | dry | IEC 60250 | 1GHz |
4 [-] Show Supplier Material materials with Dielectric constant of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.4 [-] Show Supplier Material materials with Dielectric constant of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.6 [-] Show Supplier Material materials with Dielectric constant of 4.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
12 [-] Show Supplier Material materials with Dielectric constant of 12 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Dielectric strength | 25 kV/mm Show Supplier Material materials with Dielectric strength of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Dielectric strength of 35 kV/mm | dry | IEC 60243-1 | ||
Dissipation factor | 80 [-] Show Supplier Material materials with Dissipation factor of 80 [-] | dry | IEC 62631-2-1 | 100Hz |
230 [-] Show Supplier Material materials with Dissipation factor of 230 [-] | dry | IEC 62631-2-1 | 1MHz | |
300 [-] Show Supplier Material materials with Dissipation factor of 300 [-] | dry | IEC 60250 | 1GHz | |
900 [-] Show Supplier Material materials with Dissipation factor of 900 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1500 [-] Show Supplier Material materials with Dissipation factor of 1500 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+09 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+09 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | dry | ISO 294-4 | Parallel |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 100 | dry | - | 1.0 mm 800 bar |
110 | dry | - | 1.0 mm 900 bar | |
120 | dry | - | 1.0 mm 1000 bar | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Reflow connectors, Audio Jack Connectors | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |