Límite elástico Rp 0,2: 479 - 523 MPa

Quick Comparison

Acero bajo en carbono

EN 10025-2 Grade E360 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

EN 10149-2 Grade S550MC thermomechanically rolled

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QH quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10028-6 Grade P500QH quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A572 Grade 290

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Suministrada por:

3 proveedores de Matmatch

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Suministrada por:

3 proveedores de Matmatch

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

7000 Serie

AA Standards Grade 7075 T6

Suministrada por:

3 proveedores de Matmatch

7000 Serie

AA Standards Grade 7075 T651

Suministrada por:

3 proveedores de Matmatch

Página 1 de 28