General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.3 % Show Supplier Material materials with Absorción de agua of 0.3 % | dry | Sim. to ISO 62 |
Densidad | 1.55 g/cm³ Show Supplier Material materials with Densidad of 1.55 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.4 % Show Supplier Material materials with Elongación of 2.4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 227 MPa Show Supplier Material materials with Flexural yield strength of 227 MPa | dry | ISO 178 | |
Módulo de flexión | 9.2 GPa Show Supplier Material materials with Módulo de flexión of 9.2 GPa | dry | ISO 178 | |
Módulo elástico | 9.9 GPa Show Supplier Material materials with Módulo elástico of 9.9 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry | ISO 179/1eU |
23 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | dry | ISO 75-1/-2 | 2 MPa | |
225 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 225 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.9 [-] Show Supplier Material materials with Constante dieléctrica of 3.9 [-] | dry | IEC 62631-2-1 | 1MHz |
4.1 [-] Show Supplier Material materials with Constante dieléctrica of 4.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 15 [-] Show Supplier Material materials with Factor de disipación of 15 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Factor de disipación of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 275 V Show Supplier Material materials with Índice de seguimiento comparativo of 275 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |