General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.2 % Show Supplier Material materials with Absorción de agua of 4.2 % | dry | Sim. to ISO 62 |
Densidad | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 |
2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | ||
3.9 % Show Supplier Material materials with Elongación of 3.9 % | conditioned | ISO 527-1/-2 | ||
120 °C | 5.1 % Show Supplier Material materials with Elongación of 5.1 % | dry | ISO 527-1/-2 | |
140 °C | 5.3 % Show Supplier Material materials with Elongación of 5.3 % | dry | ISO 527-1/-2 | |
150 °C | 5.4 % Show Supplier Material materials with Elongación of 5.4 % | dry | ISO 527-1/-2 | |
160 °C | 5.5 % Show Supplier Material materials with Elongación of 5.5 % | dry | ISO 527-1/-2 | |
180 °C | 5.7 % Show Supplier Material materials with Elongación of 5.7 % | dry | ISO 527-1/-2 | |
200 °C | 5.9 % Show Supplier Material materials with Elongación of 5.9 % | dry | ISO 527-1/-2 | |
210 °C | 0.006 % Show Supplier Material materials with Elongación of 0.006 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 275 MPa Show Supplier Material materials with Flexural yield strength of 275 MPa | conditioned | ISO 178 | |
350 MPa Show Supplier Material materials with Flexural yield strength of 350 MPa | dry | ISO 178 | ||
120 °C | 175 MPa Show Supplier Material materials with Flexural yield strength of 175 MPa | dry | ISO 178 | |
160 °C | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | dry | ISO 178 | |
180 °C | 128 MPa Show Supplier Material materials with Flexural yield strength of 128 MPa | dry | ISO 178 | |
200 °C | 115 MPa Show Supplier Material materials with Flexural yield strength of 115 MPa | dry | ISO 178 | |
210 °C | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
Módulo de flexión | 11.5 GPa Show Supplier Material materials with Módulo de flexión of 11.5 GPa | conditioned | ISO 178 | |
15.5 GPa Show Supplier Material materials with Módulo de flexión of 15.5 GPa | dry | ISO 178 | ||
120 °C | 8 GPa Show Supplier Material materials with Módulo de flexión of 8 GPa | dry | ISO 178 | |
160 °C | 7 GPa Show Supplier Material materials with Módulo de flexión of 7 GPa | dry | ISO 178 | |
180 °C | 6.5 GPa Show Supplier Material materials with Módulo de flexión of 6.5 GPa | dry | ISO 178 | |
200 °C | 6.1 GPa Show Supplier Material materials with Módulo de flexión of 6.1 GPa | dry | ISO 178 | |
210 °C | 5.8 GPa Show Supplier Material materials with Módulo de flexión of 5.8 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 16.5 GPa Show Supplier Material materials with Módulo elástico of 16.5 GPa | dry | ISO 527-1/-2 |
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | conditioned | ISO 527-1/-2 | ||
16 GPa Show Supplier Material materials with Módulo elástico of 16 GPa | dry | ISO 527-1/-2 | ||
40 °C | 15 GPa Show Supplier Material materials with Módulo elástico of 15 GPa | dry | ISO 527-1/-2 | |
100 °C | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |
120 °C | 7.4 GPa Show Supplier Material materials with Módulo elástico of 7.4 GPa | dry | ISO 527-1/-2 | |
140 °C | 6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | dry | ISO 527-1/-2 | |
150 °C | 6.6 GPa Show Supplier Material materials with Módulo elástico of 6.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 6.3 GPa Show Supplier Material materials with Módulo elástico of 6.3 GPa | dry | ISO 527-1/-2 | |
180 °C | 5.7 GPa Show Supplier Material materials with Módulo elástico of 5.7 GPa | dry | ISO 527-1/-2 | |
200 °C | 5.2 GPa Show Supplier Material materials with Módulo elástico of 5.2 GPa | dry | ISO 527-1/-2 | |
210 °C | 4.9 GPa Show Supplier Material materials with Módulo elástico of 4.9 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 300 MPa Show Supplier Material materials with Resistencia a la tracción of 300 MPa | dry | ISO 527-1/-2 |
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | conditioned | ISO 527-1/-2 | ||
240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | dry | ISO 527-1/-2 | ||
100 °C | 135 MPa Show Supplier Material materials with Resistencia a la tracción of 135 MPa | dry | ISO 527-1/-2 | |
120 °C | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-1/-2 | |
140 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
150 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | dry | ISO 527-1/-2 | |
160 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
180 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | dry | ISO 527-1/-2 | |
200 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | |
210 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry | ISO 179/1eA | |
23 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 21 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 97 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 97 kJ/m² | dry | ISO 179/1eU |
-30 °C | 101 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 101 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 94 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 94 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 253 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 253 °C | dry | ISO 75-1/-2 | 2 MPa | |
260 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 260 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Front End Modules, Timing drive systems | |
Fillers | 50% Glass Fiber |