General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 10 % Show Supplier Material materials with Absorción de agua of 10 % | dry | Sim. to ISO 62 |
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Índice límite de óxigeno | 26 % Show Supplier Material materials with Índice límite de óxigeno of 26 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 11 % Show Supplier Material materials with Elongación of 11 % | dry | ISO 527-1/-2 |
20 % Show Supplier Material materials with Elongación of 20 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | -40 °C | 7.2 % Show Supplier Material materials with Elongation at yield of 7.2 % | dry | ISO 527-1/-2 |
4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | ||
25 % Show Supplier Material materials with Elongation at yield of 25 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 35 MPa Show Supplier Material materials with Flexural yield strength of 35 MPa | conditioned | ISO 178 | |
120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | ||
Límite elástico | -40 °C | 122 MPa Show Supplier Material materials with Límite elástico of 122 MPa | dry | ISO 527-1/-2 |
45 MPa Show Supplier Material materials with Límite elástico of 45 MPa | conditioned | ISO 527-1/-2 | ||
87 MPa Show Supplier Material materials with Límite elástico of 87 MPa | dry | ISO 527-1/-2 | ||
Módulo de flexión | 0.9 GPa Show Supplier Material materials with Módulo de flexión of 0.9 GPa | conditioned | ISO 178 | |
2.9 GPa Show Supplier Material materials with Módulo de flexión of 2.9 GPa | dry | ISO 178 | ||
Módulo elástico | -40 °C | 3.5 GPa Show Supplier Material materials with Módulo elástico of 3.5 GPa | dry | ISO 527-1/-2 |
1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | conditioned | ISO 527-1/-2 | ||
3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | dry | ISO 527-1/-2 | ||
100 °C | 0.5 GPa Show Supplier Material materials with Módulo elástico of 0.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | dry | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.5 kJ/m² | dry | ISO 179/1eA |
-30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 4.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 35 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 205 °C Show Supplier Material materials with Ball pressure temperature of 205 °C | dry | IEC 60695-10-2 | |||
Coeficiente de dilatación térmica | 9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 8.82e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 8.82e-08 mm²/s | dry | - | |||
Glow Wire Flammability Index | 875 °C Show Supplier Material materials with Glow Wire Flammability Index of 875 °C | dry | IEC 60695-2-12 | 0.75 mm | ||
900 °C Show Supplier Material materials with Glow Wire Flammability Index of 900 °C | dry | IEC 60695-2-12 | 2 mm | |||
Inflamabilidad | V-2 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 60 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 °C | dry | ISO 75-1/-2 | 2 MPa | ||
160 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 160 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.1 [-] Show Supplier Material materials with Constante dieléctrica of 3.1 [-] | dry | IEC 62631-2-1 | 1MHz |
3.4 [-] Show Supplier Material materials with Constante dieléctrica of 3.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.7 [-] Show Supplier Material materials with Constante dieléctrica of 4.7 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
15 [-] Show Supplier Material materials with Constante dieléctrica of 15 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 65 [-] Show Supplier Material materials with Factor de disipación of 65 [-] | dry | IEC 62631-2-1 | 100Hz |
165 [-] Show Supplier Material materials with Factor de disipación of 165 [-] | dry | IEC 62631-2-1 | 1MHz | |
1300 [-] Show Supplier Material materials with Factor de disipación of 1300 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3900 [-] Show Supplier Material materials with Factor de disipación of 3900 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | conditioned | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Parallel | |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Normal | ||
Density of melt | 960 g/cm³ Show Supplier Material materials with Density of melt of 960 g/cm³ | dry | - | ||
Specific heat capacity melt | 2680 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2680 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.23 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.23 W/(m·K) | dry | - | ||
Velocidad de flujo de la masa derretida | 260 °C | 44 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 44 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 260 °C | 44 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 44 cm³/10min | dry | ISO 1133 | |
Viscosity number | 132 cm³/gr Show Supplier Material materials with Viscosity number of 132 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Wall plates, CEE connectors, Industrial Connectors, EV Charging Connectors, Terminal Blocks | |
Certifications | Food Contact, Yellow Card Available |