General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Densidad | 1.28 g/cm³ Show Supplier Material materials with Densidad of 1.28 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | dry | ISO 178 | |
Módulo de flexión | 7.5 GPa Show Supplier Material materials with Módulo de flexión of 7.5 GPa | dry | ISO 178 | |
Módulo elástico | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 2 MPa | |
240 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 240 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.28 [-] Show Supplier Material materials with Constante dieléctrica of 3.28 [-] | dry | IEC 60250 | 10GHz |
3.29 [-] Show Supplier Material materials with Constante dieléctrica of 3.29 [-] | dry | IEC 60250 | 5GHz | |
3.33 [-] Show Supplier Material materials with Constante dieléctrica of 3.33 [-] | dry | IEC 60250 | 1GHz | |
3.74 [-] Show Supplier Material materials with Constante dieléctrica of 3.74 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.38 [-] Show Supplier Material materials with Constante dieléctrica of 4.38 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 80 [-] Show Supplier Material materials with Factor de disipación of 80 [-] | dry | IEC 60250 | 10GHz |
100 [-] Show Supplier Material materials with Factor de disipación of 100 [-] | dry | IEC 60250 | 5GHz | |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | dry | IEC 60250 | 1GHz | |
200 [-] Show Supplier Material materials with Factor de disipación of 200 [-] | dry | IEC 62631-2-1 | 100Hz | |
240 [-] Show Supplier Material materials with Factor de disipación of 240 [-] | dry | IEC 62631-2-1 | 1MHz |
Technological properties
Property | ||
---|---|---|
Fillers | 25% Glass Fiber |