General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 1.9 % Show Supplier Material materials with Absorción de agua of 1.9 % | dry | ISO 62 | at 23°C after 24h |
6.75 % Show Supplier Material materials with Absorción de agua of 6.75 % | dry | Sim. to ISO 62 | ||
Densidad | 1.62 g/cm³ Show Supplier Material materials with Densidad of 1.62 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.85 % Show Supplier Material materials with Moisture absorption of 1.85 % | dry | Sim. to ISO 62 | |
Índice límite de óxigeno | 22 % Show Supplier Material materials with Índice límite de óxigeno of 22 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 |
2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | ||
5 % Show Supplier Material materials with Elongación of 5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
140 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
150 °C | 5.5 % Show Supplier Material materials with Elongación of 5.5 % | dry | ISO 527-1/-2 | |
160 °C | 5.5 % Show Supplier Material materials with Elongación of 5.5 % | dry | ISO 527-1/-2 | |
180 °C | 5.5 % Show Supplier Material materials with Elongación of 5.5 % | dry | ISO 527-1/-2 | |
200 °C | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |
210 °C | 0.006 % Show Supplier Material materials with Elongación of 0.006 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |
380 MPa Show Supplier Material materials with Flexural yield strength of 380 MPa | dry | ISO 178 | ||
120 °C | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |
160 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
Módulo de flexión | 9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | conditioned | ISO 178 | |
15 GPa Show Supplier Material materials with Módulo de flexión of 15 GPa | dry | ISO 178 | ||
120 °C | 7.3 GPa Show Supplier Material materials with Módulo de flexión of 7.3 GPa | dry | ISO 178 | |
160 °C | 6.5 GPa Show Supplier Material materials with Módulo de flexión of 6.5 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 16.5 GPa Show Supplier Material materials with Módulo elástico of 16.5 GPa | dry | ISO 527-1/-2 |
10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | conditioned | ISO 527-1/-2 | ||
16 GPa Show Supplier Material materials with Módulo elástico of 16 GPa | dry | ISO 527-1/-2 | ||
100 °C | 9.5 GPa Show Supplier Material materials with Módulo elástico of 9.5 GPa | dry | ISO 527-1/-2 | |
120 °C | 8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | dry | ISO 527-1/-2 | |
140 °C | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |
150 °C | 7.6 GPa Show Supplier Material materials with Módulo elástico of 7.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 7.2 GPa Show Supplier Material materials with Módulo elástico of 7.2 GPa | dry | ISO 527-1/-2 | |
180 °C | 6.6 GPa Show Supplier Material materials with Módulo elástico of 6.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 6 GPa Show Supplier Material materials with Módulo elástico of 6 GPa | dry | ISO 527-1/-2 | |
210 °C | 5.8 GPa Show Supplier Material materials with Módulo elástico of 5.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 290 MPa Show Supplier Material materials with Resistencia a la tracción of 290 MPa | dry | ISO 527-1/-2 |
150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | conditioned | ISO 527-1/-2 | ||
250 MPa Show Supplier Material materials with Resistencia a la tracción of 250 MPa | dry | ISO 527-1/-2 | ||
100 °C | 150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | ISO 527-1/-2 | |
120 °C | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | dry | ISO 527-1/-2 | |
140 °C | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | |
150 °C | 125 MPa Show Supplier Material materials with Resistencia a la tracción of 125 MPa | dry | ISO 527-1/-2 | |
160 °C | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-1/-2 | |
180 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
200 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
210 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry | ISO 179/1eA | |
23 °C | 24 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 24 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU |
-30 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | dry | ISO 179/1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 110 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.39e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.39e-07 mm²/s | dry | - | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.3 [-] Show Supplier Material materials with Constante dieléctrica of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.7 [-] Show Supplier Material materials with Constante dieléctrica of 4.7 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
16 [-] Show Supplier Material materials with Constante dieléctrica of 16 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 70 [-] Show Supplier Material materials with Factor de disipación of 70 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Factor de disipación of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Factor de disipación of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
6000 [-] Show Supplier Material materials with Factor de disipación of 6000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+08 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+08 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 300 V Show Supplier Material materials with Índice de seguimiento comparativo of 300 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | Sim. to ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1420.0 g/cm³ Show Supplier Material materials with Density of melt of 1420.0 g/cm³ | dry | - | |
Specific heat capacity melt | 1990 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1990 J/(kg·K) | dry | - | |
Spiral flow length | 70 | dry | - | 1.0 mm 800 bar |
80 | dry | - | 1.0 mm 900 bar | |
90 | dry | - | 1.0 mm 1000 bar | |
Thermal conductivity of melt | 0.391 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.391 W/(m·K) | dry | - | |
Viscosity number | 140 cm³/gr Show Supplier Material materials with Viscosity number of 140 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Off-road Vehicle Oil Pans and Reservoirs, MTF/DMF Components, Torque Convertor Components, Charge Air Cooler Caps, EPS Steering components: Gears, Flex couplers and Sensors, Wheel Speed Sensors, Endlaminates (electrical components), Gears, Timing drive systems, Electric parking brakes, Electric brake boosters, Electronic throttle control actuators, Exhaust gas recirculation actuators, Turbo actuators, Coolant valve actuators, Seat actuators, Mirror actuators, Trunk actuators, Door handle actuators, Sunroof actuators, Steering wheel adjusters | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |