Akulon® S223-G6-FC NA99001

Nombres alternativos y comerciales
PA66-GF30
Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® S223-G6-FC NA99001

Los datos sobre este material han sido proporcionados por DSM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueConditionTesting Standard

Absorción de agua

6 %

Show Supplier Material materials with Absorción de agua of 6 %

dry

Sim. to ISO 62

Densidad

1.36 g/cm³

Show Supplier Material materials with Densidad of 1.36 g/cm³

dry

ISO 1183

Moisture absorption

1.6 %

Show Supplier Material materials with Moisture absorption of 1.6 %

dry

Sim. to ISO 62

Mecánica

PropertyTemperatureValueConditionTesting Standard

Elongación

3 %

Show Supplier Material materials with Elongación of 3 %

dry

ISO 527-1/-2

5 %

Show Supplier Material materials with Elongación of 5 %

conditioned

ISO 527-1/-2

Flexural yield strength

250 MPa

Show Supplier Material materials with Flexural yield strength of 250 MPa

dry

ISO 178

Módulo de flexión

8.4 GPa

Show Supplier Material materials with Módulo de flexión of 8.4 GPa

dry

ISO 178

Módulo elástico

7.5 GPa

Show Supplier Material materials with Módulo elástico of 7.5 GPa

conditioned

ISO 527-1/-2

9.5 GPa

Show Supplier Material materials with Módulo elástico of 9.5 GPa

dry

ISO 527-1/-2

Resistencia a la tracción

140 MPa

Show Supplier Material materials with Resistencia a la tracción of 140 MPa

conditioned

ISO 527-1/-2

190 MPa

Show Supplier Material materials with Resistencia a la tracción of 190 MPa

dry

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-30 °C

10 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m²

dry, conditioned

ISO 179/1eA

23 °C

12 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m²

dry

ISO 179/1eA

23 °C

20 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m²

conditioned

ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

-30 °C

70 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m²

dry, conditioned

ISO 179/1eU

23 °C

80 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m²

dry

ISO 179/1eU

23 °C

100 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m²

conditioned

ISO 179/1eU

Aplicaciones térmicas

PropertyValueConditionTesting StandardThicknessPressureComment

Coeficiente de dilatación térmica

2e-07 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K

dry

ISO 11359-1/-2

Parallel

7e-07 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K

dry

ISO 11359-1/-2

Normal

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

dry

UL746B

0.71 mm

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

dry

UL746B

0.71 mm

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

dry

UL746B

0.71 mm

Temperatura de flexión bajo carga

245 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 245 °C

dry

ISO 75-1/-2

2 MPa

260 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 260 °C

dry

ISO 75-1/-2

0.45 MPa

Temperatura de fusión

260 °C

Show Supplier Material materials with Temperatura de fusión of 260 °C

dry

ISO 11357-1/-3

10°C/min

Eléctrico

PropertyValueConditionTesting StandardComment

Constante dieléctrica

3.5 [-]

Show Supplier Material materials with Constante dieléctrica of 3.5 [-]

dry

IEC 62631-2-1

1MHz

3.8 [-]

Show Supplier Material materials with Constante dieléctrica of 3.8 [-]

dry

IEC 62631-2-1

100Hz

4.6 [-]

Show Supplier Material materials with Constante dieléctrica of 4.6 [-]

conditioned

IEC 62631-2-1

1MHz

11 [-]

Show Supplier Material materials with Constante dieléctrica of 11 [-]

conditioned

IEC 62631-2-1

100Hz

Factor de disipación

90 [-]

Show Supplier Material materials with Factor de disipación of 90 [-]

dry

IEC 62631-2-1

100Hz

160 [-]

Show Supplier Material materials with Factor de disipación of 160 [-]

dry

IEC 62631-2-1

1MHz

1000 [-]

Show Supplier Material materials with Factor de disipación of 1000 [-]

conditioned

IEC 62631-2-1

1MHz

1400 [-]

Show Supplier Material materials with Factor de disipación of 1400 [-]

conditioned

IEC 62631-2-1

100Hz

Rigidez dieléctrica

25 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm

conditioned

IEC 60243-1

30 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm

dry

IEC 60243-1

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

conditioned

IEC 62631-3-2

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

conditioned

IEC 62631-3-1

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

dry

IEC 62631-3-1

Índice de seguimiento comparativo

600 V

Show Supplier Material materials with Índice de seguimiento comparativo of 600 V

dry, conditioned

IEC 60112

Rheological Properties

PropertyValueConditionTesting StandardComment

Contracción

0.2 %

Show Supplier Material materials with Contracción of 0.2 %

dry

Sim. to ISO 294-4

Parallel

1.2 %

Show Supplier Material materials with Contracción of 1.2 %

dry

Sim. to ISO 294-4

Normal

Specific heat capacity melt

2170 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2170 J/(kg·K)

dry

-

Thermal conductivity of melt

0.172 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.172 W/(m·K)

dry

-

Technological properties

Property
Application areas

Spatulas and Kitchenware

Certifications

Food Contact

Fillers

30% Glass Fiber