General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 41 % Show Supplier Material materials with Bio-based content of 41 % | dry | ASTM D6866-12 Method B |
Densidad | 1.34 g/cm³ Show Supplier Material materials with Densidad of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
Módulo elástico | 6.4 GPa Show Supplier Material materials with Módulo elástico of 6.4 GPa | conditioned | ISO 527-1/-2 | |
9 GPa Show Supplier Material materials with Módulo elástico of 9 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | conditioned | ISO 527-1/-2 | |
165 MPa Show Supplier Material materials with Resistencia a la tracción of 165 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 9.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |