Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 6 % Show Supplier Material materials with Absorción de agua of 6 % | dry | Sim. to ISO 62 |
Densidad | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 235 MPa Show Supplier Material materials with Flexural yield strength of 235 MPa | dry | ISO 178 | |
Módulo de flexión | 8.6 GPa Show Supplier Material materials with Módulo de flexión of 8.6 GPa | dry | ISO 178 | |
Módulo elástico | 5.7 GPa Show Supplier Material materials with Módulo elástico of 5.7 GPa | conditioned | ISO 527-1/-2 | |
9.5 GPa Show Supplier Material materials with Módulo elástico of 9.5 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | dry | ISO 179/1eA | |
23 °C | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 22 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | dry | ISO 179/1eU | |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 1.08e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.08e-07 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel | |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Normal | ||
Density of melt | 1120 g/cm³ Show Supplier Material materials with Density of melt of 1120 g/cm³ | dry | - | ||
Specific heat capacity melt | 2250 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2250 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - | ||
Velocidad de flujo de la masa derretida | 275 °C | 55.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 55.0 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |