General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.34 g/cm³ Show Supplier Material materials with Densidad of 1.34 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Elongación | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | ||
12 % Show Supplier Material materials with Elongación of 12 % | dry | ISO 527-1/-2 | 1 mm | ||
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | |||
60 % Show Supplier Material materials with Elongación of 60 % | conditioned | ISO 527-1/-2 | |||
120 °C | 150 % Show Supplier Material materials with Elongación of 150 % | dry | ISO 527-1/-2 | ||
160 °C | 200 % Show Supplier Material materials with Elongación of 200 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 3.9 % Show Supplier Material materials with Elongation at yield of 3.9 % | dry | ISO 527-1/-2 | ||
14.0 % Show Supplier Material materials with Elongation at yield of 14.0 % | conditioned | ISO 527-1/-2 | |||
Flexural yield strength | 55.0 MPa Show Supplier Material materials with Flexural yield strength of 55.0 MPa | conditioned | ISO 178 | ||
125 MPa Show Supplier Material materials with Flexural yield strength of 125 MPa | dry | ISO 178 | |||
120 °C | 28.0 MPa Show Supplier Material materials with Flexural yield strength of 28.0 MPa | dry | ISO 178 | ||
160 °C | 24 MPa Show Supplier Material materials with Flexural yield strength of 24 MPa | dry | ISO 178 | ||
Módulo de flexión | 1.6 GPa Show Supplier Material materials with Módulo de flexión of 1.6 GPa | conditioned | ISO 178 | ||
3.6 GPa Show Supplier Material materials with Módulo de flexión of 3.6 GPa | dry | ISO 178 | |||
120 °C | 0.7 GPa Show Supplier Material materials with Módulo de flexión of 0.7 GPa | dry | ISO 178 | ||
160 °C | 0.6 GPa Show Supplier Material materials with Módulo de flexión of 0.6 GPa | dry | ISO 178 | ||
Módulo elástico | 1.4 GPa Show Supplier Material materials with Módulo elástico of 1.4 GPa | conditioned | ISO 527-1/-2 | ||
1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | conditioned | ISO 527-1/-2 | |||
3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | dry | ISO 527-1/-2 | 1 mm | ||
3.7 GPa Show Supplier Material materials with Módulo elástico of 3.7 GPa | dry | ISO 527-1/-2 | |||
120 °C | 0.72 GPa Show Supplier Material materials with Módulo elástico of 0.72 GPa | dry | ISO 527-1/-2 | ||
160 °C | 0.58 GPa Show Supplier Material materials with Módulo elástico of 0.58 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 3.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | conditioned | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 245 °C Show Supplier Material materials with Ball pressure temperature of 245 °C | dry | IEC 60695-10-2 | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.4 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 960 °C | dry | IEC 60695-2-13 | 0.4 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | dry | UL746B | 0.4 mm | ||
Relative temperature index, mechanical impact | 100 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 100 °C | dry | UL746B | 0.4 mm | ||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | dry | UL746B | 0.4 mm | ||
Temperatura de flexión bajo carga | 85 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 85 °C | dry | ISO 75-1/-2 | 2 MPa | ||
225 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 225 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 250 V Show Supplier Material materials with Índice de seguimiento comparativo of 250 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Appliance connector | |
Certifications | Yellow Card Available |