General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.1 % Show Supplier Material materials with Absorción de agua of 4.1 % | dry | Sim. to ISO 62 |
Densidad | 1.49 g/cm³ Show Supplier Material materials with Densidad of 1.49 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Elongación | -40 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | ||
2.4 % Show Supplier Material materials with Elongación of 2.4 % | conditioned | ISO 527-1/-2 | ||||
2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | ||||
2.8 % Show Supplier Material materials with Elongación of 2.8 % | dry | ISO 527-1/-2 | 1 mm | |||
40 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |||
80 °C | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | |||
100 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | |||
100 °C | 6.6 % Show Supplier Material materials with Elongación of 6.6 % | conditioned | ISO 527-1/-2 | |||
120 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | dry | ISO 527-1/-2 | |||
120 °C | 6.3 % Show Supplier Material materials with Elongación of 6.3 % | conditioned | ISO 527-1/-2 | |||
150 °C | 8 % Show Supplier Material materials with Elongación of 8 % | dry | ISO 527-1/-2 | |||
180 °C | 8 % Show Supplier Material materials with Elongación of 8 % | dry | ISO 527-1/-2 | |||
200 °C | 8 % Show Supplier Material materials with Elongación of 8 % | dry | ISO 527-1/-2 | |||
210 °C | 0.007 % Show Supplier Material materials with Elongación of 0.007 % | dry | ISO 527-1/-2 | |||
Flexural yield strength | 290 MPa Show Supplier Material materials with Flexural yield strength of 290 MPa | conditioned | ISO 178 | |||
320 MPa Show Supplier Material materials with Flexural yield strength of 320 MPa | dry | ISO 178 | ||||
120 °C | 220 MPa Show Supplier Material materials with Flexural yield strength of 220 MPa | dry | ISO 178 | |||
160 °C | 93 MPa Show Supplier Material materials with Flexural yield strength of 93 MPa | dry | ISO 178 | |||
180 °C | 83 MPa Show Supplier Material materials with Flexural yield strength of 83 MPa | dry | ISO 178 | |||
200 °C | 77 MPa Show Supplier Material materials with Flexural yield strength of 77 MPa | dry | ISO 178 | |||
210 °C | 72 MPa Show Supplier Material materials with Flexural yield strength of 72 MPa | dry | ISO 178 | |||
Módulo de flexión | 12 GPa Show Supplier Material materials with Módulo de flexión of 12 GPa | dry | ISO 178 | |||
12.5 GPa Show Supplier Material materials with Módulo de flexión of 12.5 GPa | conditioned | ISO 178 | ||||
120 °C | 10.9 GPa Show Supplier Material materials with Módulo de flexión of 10.9 GPa | dry | ISO 178 | |||
160 °C | 4.3 GPa Show Supplier Material materials with Módulo de flexión of 4.3 GPa | dry | ISO 178 | |||
180 °C | 3.9 GPa Show Supplier Material materials with Módulo de flexión of 3.9 GPa | dry | ISO 178 | |||
200 °C | 3.7 GPa Show Supplier Material materials with Módulo de flexión of 3.7 GPa | dry | ISO 178 | |||
210 °C | 3.6 GPa Show Supplier Material materials with Módulo de flexión of 3.6 GPa | dry | ISO 178 | |||
Módulo elástico | -40 °C | 12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | dry | ISO 527-1/-2 | ||
12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | ISO 527-1/-2 | 1 mm | |||
12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | dry | ISO 527-1/-2 | ||||
12.9 GPa Show Supplier Material materials with Módulo elástico of 12.9 GPa | conditioned | ISO 527-1/-2 | ||||
40 °C | 12.2 GPa Show Supplier Material materials with Módulo elástico of 12.2 GPa | dry | ISO 527-1/-2 | |||
80 °C | 11.9 GPa Show Supplier Material materials with Módulo elástico of 11.9 GPa | dry | ISO 527-1/-2 | |||
100 °C | 5 GPa Show Supplier Material materials with Módulo elástico of 5 GPa | conditioned | ISO 527-1/-2 | |||
100 °C | 11.6 GPa Show Supplier Material materials with Módulo elástico of 11.6 GPa | dry | ISO 527-1/-2 | |||
120 °C | 4.6 GPa Show Supplier Material materials with Módulo elástico of 4.6 GPa | conditioned | ISO 527-1/-2 | |||
120 °C | 11.2 GPa Show Supplier Material materials with Módulo elástico of 11.2 GPa | dry | ISO 527-1/-2 | |||
150 °C | 5.3 GPa Show Supplier Material materials with Módulo elástico of 5.3 GPa | dry | ISO 527-1/-2 | |||
160 °C | 4.6 GPa Show Supplier Material materials with Módulo elástico of 4.6 GPa | dry | ISO 527-1/-2 | |||
180 °C | 4 GPa Show Supplier Material materials with Módulo elástico of 4 GPa | dry | ISO 527-1/-2 | |||
200 °C | 3.7 GPa Show Supplier Material materials with Módulo elástico of 3.7 GPa | dry | ISO 527-1/-2 | |||
210 °C | 3.5 GPa Show Supplier Material materials with Módulo elástico of 3.5 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | -40 °C | 260 MPa Show Supplier Material materials with Resistencia a la tracción of 260 MPa | dry | ISO 527-1/-2 | ||
220 MPa Show Supplier Material materials with Resistencia a la tracción of 220 MPa | conditioned | ISO 527-1/-2 | ||||
230 MPa Show Supplier Material materials with Resistencia a la tracción of 230 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | dry | ISO 527-1/-2 | ||||
40 °C | 220 MPa Show Supplier Material materials with Resistencia a la tracción of 220 MPa | dry | ISO 527-1/-2 | |||
80 °C | 190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | dry | ISO 527-1/-2 | |||
100 °C | 76 MPa Show Supplier Material materials with Resistencia a la tracción of 76 MPa | conditioned | ISO 527-1/-2 | |||
100 °C | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | ISO 527-1/-2 | |||
120 °C | 68 MPa Show Supplier Material materials with Resistencia a la tracción of 68 MPa | conditioned | ISO 527-1/-2 | |||
120 °C | 145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | dry | ISO 527-1/-2 | |||
150 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | dry | ISO 527-1/-2 | |||
160 °C | 78 MPa Show Supplier Material materials with Resistencia a la tracción of 78 MPa | dry | ISO 527-1/-2 | |||
180 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | dry | ISO 527-1/-2 | |||
200 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |||
210 °C | 51 MPa Show Supplier Material materials with Resistencia a la tracción of 51 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | conditioned | ISO 179/1eA | ||
-30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |||
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | conditioned | ISO 179/1eA | |||
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 72 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 72 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 76 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 76 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5.1e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.1e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 300 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 300 °C | dry | ISO 75-1/-2 | 2 MPa | |
315 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 315 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 330 °C Show Supplier Material materials with Temperatura de fusión of 330 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 145 °C Show Supplier Material materials with Temperatura de transición del vidrio of 145 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | dry, conditioned | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Coolant connectors, Engine water jackets, Thermal management modules | |
Fillers | 35% Glass Fiber |