General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5 % Show Supplier Material materials with Absorción de agua of 5 % | dry | Sim. to ISO 62 |
Densidad | 1.41 g/cm³ Show Supplier Material materials with Densidad of 1.41 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | ISO 527-1/-2 |
3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | ISO 527-1/-2 | ||
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
120 °C | 9.2 % Show Supplier Material materials with Elongación of 9.2 % | dry | ISO 527-1/-2 | |
150 °C | 9.6 % Show Supplier Material materials with Elongación of 9.6 % | dry | ISO 527-1/-2 | |
160 °C | 9.6 % Show Supplier Material materials with Elongación of 9.6 % | dry | ISO 527-1/-2 | |
180 °C | 9.6 % Show Supplier Material materials with Elongación of 9.6 % | dry | ISO 527-1/-2 | |
200 °C | 9.6 % Show Supplier Material materials with Elongación of 9.6 % | dry | ISO 527-1/-2 | |
210 °C | 0.01 % Show Supplier Material materials with Elongación of 0.01 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 175 MPa Show Supplier Material materials with Flexural yield strength of 175 MPa | conditioned | ISO 178 | |
290 MPa Show Supplier Material materials with Flexural yield strength of 290 MPa | dry | ISO 178 | ||
120 °C | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | dry | ISO 178 | |
160 °C | 105 MPa Show Supplier Material materials with Flexural yield strength of 105 MPa | dry | ISO 178 | |
180 °C | 95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | |
200 °C | 80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | dry | ISO 178 | |
210 °C | 75 MPa Show Supplier Material materials with Flexural yield strength of 75 MPa | dry | ISO 178 | |
Módulo de flexión | 6.3 GPa Show Supplier Material materials with Módulo de flexión of 6.3 GPa | conditioned | ISO 178 | |
10.5 GPa Show Supplier Material materials with Módulo de flexión of 10.5 GPa | dry | ISO 178 | ||
120 °C | 4.6 GPa Show Supplier Material materials with Módulo de flexión of 4.6 GPa | dry | ISO 178 | |
160 °C | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | dry | ISO 178 | |
180 °C | 4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | dry | ISO 178 | |
200 °C | 3.6 GPa Show Supplier Material materials with Módulo de flexión of 3.6 GPa | dry | ISO 178 | |
210 °C | 3.3 GPa Show Supplier Material materials with Módulo de flexión of 3.3 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 11.3 GPa Show Supplier Material materials with Módulo elástico of 11.3 GPa | dry | ISO 527-1/-2 |
6.5 GPa Show Supplier Material materials with Módulo elástico of 6.5 GPa | conditioned | ISO 527-1/-2 | ||
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-1/-2 | ||
40 °C | 10.2 GPa Show Supplier Material materials with Módulo elástico of 10.2 GPa | dry | ISO 527-1/-2 | |
100 °C | 5.1 GPa Show Supplier Material materials with Módulo elástico of 5.1 GPa | dry | ISO 527-1/-2 | |
120 °C | 4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | dry | ISO 527-1/-2 | |
150 °C | 4.2 GPa Show Supplier Material materials with Módulo elástico of 4.2 GPa | dry | ISO 527-1/-2 | |
160 °C | 4.1 GPa Show Supplier Material materials with Módulo elástico of 4.1 GPa | dry | ISO 527-1/-2 | |
180 °C | 3.8 GPa Show Supplier Material materials with Módulo elástico of 3.8 GPa | dry | ISO 527-1/-2 | |
200 °C | 3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | dry | ISO 527-1/-2 | |
210 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 255 MPa Show Supplier Material materials with Resistencia a la tracción of 255 MPa | dry | ISO 527-1/-2 |
115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | conditioned | ISO 527-1/-2 | ||
195 MPa Show Supplier Material materials with Resistencia a la tracción of 195 MPa | dry | ISO 527-1/-2 | ||
100 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | dry | ISO 527-1/-2 | |
120 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |
150 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | dry | ISO 527-1/-2 | |
160 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | dry | ISO 527-1/-2 | |
180 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
200 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | dry | ISO 527-1/-2 | |
210 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | dry | ISO 179/1eU | |
23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 240 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 240 °C | dry | ISO 75-1/-2 | 2 MPa | |
258 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 258 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | ISO 294-4 | Normal | |
Density of melt | 1220 g/cm³ Show Supplier Material materials with Density of melt of 1220 g/cm³ | dry | - | |
Specific heat capacity melt | 2060 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2060 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - | |
Viscosity number | 135 cm³/gr Show Supplier Material materials with Viscosity number of 135 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Air inlet manifolds, Integrated Air Inlet Manifolds (up to 230°C), Resonators and ByPass Valves, Hot Charged Air Ducts, Charge Air Cooler Caps | |
Fillers | 35% Glass Fiber |