General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.3 % Show Supplier Material materials with Absorción de agua of 0.3 % | dry | Sim. to ISO 62 |
Densidad | 1.72 g/cm³ Show Supplier Material materials with Densidad of 1.72 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 1.6 % Show Supplier Material materials with Elongación of 1.6 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 195 MPa Show Supplier Material materials with Flexural yield strength of 195 MPa | dry | ISO 178 | |
Módulo de flexión | 15 GPa Show Supplier Material materials with Módulo de flexión of 15 GPa | dry | ISO 178 | |
Módulo elástico | 16.5 GPa Show Supplier Material materials with Módulo elástico of 16.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 155 MPa Show Supplier Material materials with Resistencia a la tracción of 155 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 9.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9.5 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | dry | ISO 75-1/-2 | 2 MPa | |
225 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 225 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |