General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2 % Show Supplier Material materials with Absorción de agua of 2 % | dry | ISO 62 | at 23°C after 24h |
7 % Show Supplier Material materials with Absorción de agua of 7 % | dry | Sim. to ISO 62 | ||
Densidad | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.9 % Show Supplier Material materials with Elongación of 2.9 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 225 MPa Show Supplier Material materials with Flexural yield strength of 225 MPa | dry | ISO 178 | |
Módulo de flexión | 7.5 GPa Show Supplier Material materials with Módulo de flexión of 7.5 GPa | dry | ISO 178 | |
Módulo elástico | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 135 MPa Show Supplier Material materials with Resistencia a la tracción of 135 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.14e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.14e-07 mm²/s | dry | - | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | ||
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | UL746B | 0.9 mm | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.9 mm | ||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | dry | UL746B | 0.9 mm | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | conditioned | IEC 60243-1 |
30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | |
Índice de seguimiento comparativo | 175 V Show Supplier Material materials with Índice de seguimiento comparativo of 175 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.2 % Show Supplier Material materials with Contracción of 1.2 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1370 g/cm³ Show Supplier Material materials with Density of melt of 1370 g/cm³ | dry | - | |
Specific heat capacity melt | 1790 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1790 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | FPC connectors, WtB and BtB Connectors, Bobbins | |
Certifications | Yellow Card Available | |
Fillers | 15% Glass Fiber |