General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | dry | ISO 62 | at 23°C after 24h |
4.8 % Show Supplier Material materials with Absorción de agua of 4.8 % | dry | Sim. to ISO 62 | ||
Densidad | 1.46 g/cm³ Show Supplier Material materials with Densidad of 1.46 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 |
2.5 % Show Supplier Material materials with Elongación of 2.5 % | conditioned | ISO 527-1/-2 | ||
2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | ||
40 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |
80 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | |
80 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | conditioned | ISO 527-1/-2 | |
100 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | |
120 °C | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-1/-2 | |
120 °C | 5 % Show Supplier Material materials with Elongación of 5 % | conditioned | ISO 527-1/-2 | |
150 °C | 3.8 % Show Supplier Material materials with Elongación of 3.8 % | dry | ISO 527-1/-2 | |
160 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
180 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
200 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
210 °C | 0.005 % Show Supplier Material materials with Elongación of 0.005 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 275 MPa Show Supplier Material materials with Flexural yield strength of 275 MPa | conditioned | ISO 178 | |
300 MPa Show Supplier Material materials with Flexural yield strength of 300 MPa | dry | ISO 178 | ||
80 °C | 190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | conditioned | ISO 178 | |
80 °C | 270 MPa Show Supplier Material materials with Flexural yield strength of 270 MPa | dry | ISO 178 | |
120 °C | 220 MPa Show Supplier Material materials with Flexural yield strength of 220 MPa | dry | ISO 178 | |
160 °C | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | dry | ISO 178 | |
180 °C | 125 MPa Show Supplier Material materials with Flexural yield strength of 125 MPa | dry | ISO 178 | |
200 °C | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
210 °C | 105 MPa Show Supplier Material materials with Flexural yield strength of 105 MPa | dry | ISO 178 | |
Módulo de flexión | 10.5 GPa Show Supplier Material materials with Módulo de flexión of 10.5 GPa | dry, conditioned | ISO 178 | |
80 °C | 9.8 GPa Show Supplier Material materials with Módulo de flexión of 9.8 GPa | conditioned | ISO 178 | |
80 °C | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | |
120 °C | 9.5 GPa Show Supplier Material materials with Módulo de flexión of 9.5 GPa | dry | ISO 178 | |
160 °C | 5.7 GPa Show Supplier Material materials with Módulo de flexión of 5.7 GPa | dry | ISO 178 | |
180 °C | 4.7 GPa Show Supplier Material materials with Módulo de flexión of 4.7 GPa | dry | ISO 178 | |
200 °C | 4.3 GPa Show Supplier Material materials with Módulo de flexión of 4.3 GPa | dry | ISO 178 | |
210 °C | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 11.8 GPa Show Supplier Material materials with Módulo elástico of 11.8 GPa | dry | ISO 527-1/-2 |
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry, conditioned | ISO 527-1/-2 | ||
40 °C | 10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | dry | ISO 527-1/-2 | |
80 °C | 9.5 GPa Show Supplier Material materials with Módulo elástico of 9.5 GPa | conditioned | ISO 527-1/-2 | |
80 °C | 10.3 GPa Show Supplier Material materials with Módulo elástico of 10.3 GPa | dry | ISO 527-1/-2 | |
100 °C | 10.2 GPa Show Supplier Material materials with Módulo elástico of 10.2 GPa | dry | ISO 527-1/-2 | |
120 °C | 5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | conditioned | ISO 527-1/-2 | |
120 °C | 9.6 GPa Show Supplier Material materials with Módulo elástico of 9.6 GPa | dry | ISO 527-1/-2 | |
150 °C | 7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 6.3 GPa Show Supplier Material materials with Módulo elástico of 6.3 GPa | dry | ISO 527-1/-2 | |
180 °C | 4.9 GPa Show Supplier Material materials with Módulo elástico of 4.9 GPa | dry | ISO 527-1/-2 | |
200 °C | 4.4 GPa Show Supplier Material materials with Módulo elástico of 4.4 GPa | dry | ISO 527-1/-2 | |
210 °C | 4.3 GPa Show Supplier Material materials with Módulo elástico of 4.3 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | dry | ISO 527-1/-2 |
190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | conditioned | ISO 527-1/-2 | ||
210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | dry | ISO 527-1/-2 | ||
40 °C | 200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | |
80 °C | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | conditioned | ISO 527-1/-2 | |
80 °C | 180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | ISO 527-1/-2 | |
100 °C | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | ISO 527-1/-2 | |
120 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | conditioned | ISO 527-1/-2 | |
120 °C | 150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | ISO 527-1/-2 | |
150 °C | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | dry | ISO 527-1/-2 | |
160 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
200 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | |
210 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU | |
23 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 320 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 320 °C | dry | ISO 75-1/-2 | 2 MPa | |
335 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 335 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 340 °C Show Supplier Material materials with Temperatura de fusión of 340 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 160 °C Show Supplier Material materials with Temperatura de transición del vidrio of 160 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 45 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 45 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Faucet mixing valve, Panhandle | |
Certifications | Food Contact, Drinking Water, Yellow Card Available | |
Fillers | 30% Glass Fiber |