General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 6 % Show Supplier Material materials with Absorción de agua of 6 % | dry | Sim. to ISO 62 |
Densidad | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 |
3.3 % Show Supplier Material materials with Elongación of 3.3 % | dry | ISO 527-1/-2 | ||
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
120 °C | 9.3 % Show Supplier Material materials with Elongación of 9.3 % | dry | ISO 527-1/-2 | |
150 °C | 8.9 % Show Supplier Material materials with Elongación of 8.9 % | dry | ISO 527-1/-2 | |
160 °C | 8.8 % Show Supplier Material materials with Elongación of 8.8 % | dry | ISO 527-1/-2 | |
180 °C | 8.6 % Show Supplier Material materials with Elongación of 8.6 % | dry | ISO 527-1/-2 | |
200 °C | 8.4 % Show Supplier Material materials with Elongación of 8.4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | conditioned | ISO 178 | |
270 MPa Show Supplier Material materials with Flexural yield strength of 270 MPa | dry | ISO 178 | ||
120 °C | 105 MPa Show Supplier Material materials with Flexural yield strength of 105 MPa | dry | ISO 178 | |
160 °C | 88 MPa Show Supplier Material materials with Flexural yield strength of 88 MPa | dry | ISO 178 | |
Módulo de flexión | 5.5 GPa Show Supplier Material materials with Módulo de flexión of 5.5 GPa | conditioned | ISO 178 | |
9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | dry | ISO 178 | ||
120 °C | 4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | dry | ISO 178 | |
160 °C | 3.7 GPa Show Supplier Material materials with Módulo de flexión of 3.7 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 |
5.7 GPa Show Supplier Material materials with Módulo elástico of 5.7 GPa | conditioned | ISO 527-1/-2 | ||
9.5 GPa Show Supplier Material materials with Módulo elástico of 9.5 GPa | dry | ISO 527-1/-2 | ||
100 °C | 4.2 GPa Show Supplier Material materials with Módulo elástico of 4.2 GPa | dry | ISO 527-1/-2 | |
120 °C | 3.9 GPa Show Supplier Material materials with Módulo elástico of 3.9 GPa | dry | ISO 527-1/-2 | |
150 °C | 3.5 GPa Show Supplier Material materials with Módulo elástico of 3.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | dry | ISO 527-1/-2 | |
180 °C | 3.0 GPa Show Supplier Material materials with Módulo elástico of 3.0 GPa | dry | ISO 527-1/-2 | |
200 °C | 2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 220 MPa Show Supplier Material materials with Resistencia a la tracción of 220 MPa | dry | ISO 527-1/-2 |
105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | conditioned | ISO 527-1/-2 | ||
175 MPa Show Supplier Material materials with Resistencia a la tracción of 175 MPa | dry | ISO 527-1/-2 | ||
100 °C | 87 MPa Show Supplier Material materials with Resistencia a la tracción of 87 MPa | dry | ISO 527-1/-2 | |
120 °C | 82 MPa Show Supplier Material materials with Resistencia a la tracción of 82 MPa | dry | ISO 527-1/-2 | |
150 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
160 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
180 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | dry | ISO 527-1/-2 | |
200 °C | 40 MPa Show Supplier Material materials with Resistencia a la tracción of 40 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 12.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 22 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | dry | ISO 179/1eU | |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 1.08e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.08e-07 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.3 [-] Show Supplier Material materials with Constante dieléctrica of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
5 [-] Show Supplier Material materials with Constante dieléctrica of 5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Constante dieléctrica of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 50 [-] Show Supplier Material materials with Factor de disipación of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Factor de disipación of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Factor de disipación of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 500 V Show Supplier Material materials with Índice de seguimiento comparativo of 500 V | conditioned | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel | |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Normal | ||
Density of melt | 1120 g/cm³ Show Supplier Material materials with Density of melt of 1120 g/cm³ | dry | - | ||
Specific heat capacity melt | 2250 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2250 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - | ||
Velocidad de flujo de la masa derretida | 275 °C | 55.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 55.0 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Air inlet manifolds, Temperature Sensor, Speed Sensor, Positition Sensor | |
Fillers | 30% Glass Fiber |