General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.6 % Show Supplier Material materials with Absorción de agua of 2.6 % | dry | ISO 62 | at 23°C after 24h |
9 % Show Supplier Material materials with Absorción de agua of 9 % | dry | Sim. to ISO 62 | ||
Densidad | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | ISO 527-1/-2 |
3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | ||
7 % Show Supplier Material materials with Elongación of 7 % | conditioned | ISO 527-1/-2 | ||
120 °C | 8.4 % Show Supplier Material materials with Elongación of 8.4 % | dry | ISO 527-1/-2 | |
160 °C | 8.9 % Show Supplier Material materials with Elongación of 8.9 % | dry | ISO 527-1/-2 | |
180 °C | 9.1 % Show Supplier Material materials with Elongación of 9.1 % | dry | ISO 527-1/-2 | |
200 °C | 9.4 % Show Supplier Material materials with Elongación of 9.4 % | dry | ISO 527-1/-2 | |
Módulo de flexión | 6 GPa Show Supplier Material materials with Módulo de flexión of 6 GPa | conditioned | ISO 178 | |
9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | dry | ISO 178 | ||
Módulo elástico | -40 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 |
Resistencia a la tracción | -40 °C | 240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | dry | ISO 527-1/-2 |
115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | conditioned | ISO 527-1/-2 | ||
205 MPa Show Supplier Material materials with Resistencia a la tracción of 205 MPa | dry | ISO 527-1/-2 | ||
120 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
160 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
180 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |
200 °C | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 18 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU |
-30 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 285 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 285 °C | dry | ISO 75-1/-2 | 2 MPa | |
290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | dry | ISO 306 | 50°C/h 50N | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | Sim. to ISO 294-4 | Normal | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |