General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.6 % Show Supplier Material materials with Absorción de agua of 0.6 % | dry | Sim. to ISO 62 |
Densidad | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 71 [-] Show Supplier Material materials with Dureza Shore D of 71 [-] | dry | ISO 868 | 3s | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | |||
Módulo elástico | 0.36 GPa Show Supplier Material materials with Módulo elástico of 0.36 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 30.8 MPa Show Supplier Material materials with Resistencia a la tracción of 30.8 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.75e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.75e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.75e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 52 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 52 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 216 °C Show Supplier Material materials with Temperatura de fusión of 216 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.75 % Show Supplier Material materials with Contracción of 1.75 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 230 °C | 28.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 28.0 g/10min | dry | ISO 1133 |