Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.04 % Show Supplier Material materials with Absorción de agua of 0.04 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.74 g/cm³ Show Supplier Material materials with Densidad of 1.74 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | dry | ISO 527-1/-2 |
2 % Show Supplier Material materials with Elongación of 2 % | dry | ISO 527-1/-2 | ||
120 °C | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | |
160 °C | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 280 MPa Show Supplier Material materials with Flexural yield strength of 280 MPa | dry | ISO 178 | |
120 °C | 138 MPa Show Supplier Material materials with Flexural yield strength of 138 MPa | dry | ISO 178 | |
160 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |
200 °C | 80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | dry | ISO 178 | |
Módulo de flexión | 14.5 GPa Show Supplier Material materials with Módulo de flexión of 14.5 GPa | dry | ISO 178 | |
120 °C | 7.2 GPa Show Supplier Material materials with Módulo de flexión of 7.2 GPa | dry | ISO 178 | |
160 °C | 5.5 GPa Show Supplier Material materials with Módulo de flexión of 5.5 GPa | dry | ISO 178 | |
200 °C | 4.8 GPa Show Supplier Material materials with Módulo de flexión of 4.8 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 15.5 GPa Show Supplier Material materials with Módulo elástico of 15.5 GPa | dry | ISO 527-1/-2 |
15 GPa Show Supplier Material materials with Módulo elástico of 15 GPa | dry | ISO 527-1/-2 | ||
120 °C | 7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 245 MPa Show Supplier Material materials with Resistencia a la tracción of 245 MPa | dry | ISO 527-1/-2 |
200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | ||
120 °C | 86 MPa Show Supplier Material materials with Resistencia a la tracción of 86 MPa | dry | ISO 527-1/-2 | |
160 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-07 1/K | dry | ISO 11359-1/-2 | parallel, above Tg | |||
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | normal, above Tg | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | UL746B | 0.4 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.4 mm | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | UL746B | 0.4 mm | ||
Temperatura de flexión bajo carga | 265 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 265 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 90 °C Show Supplier Material materials with Temperatura de transición del vidrio of 90 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Índice de seguimiento comparativo | 175 V Show Supplier Material materials with Índice de seguimiento comparativo of 175 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber |