General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.05 % Show Supplier Material materials with Absorción de agua of 0.05 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 |
2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | ||
120 °C | 7 % Show Supplier Material materials with Elongación of 7 % | dry | ISO 527-1/-2 | |
160 °C | 8.6 % Show Supplier Material materials with Elongación of 8.6 % | dry | ISO 527-1/-2 | |
200 °C | 9.1 % Show Supplier Material materials with Elongación of 9.1 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 210 MPa Show Supplier Material materials with Flexural yield strength of 210 MPa | dry | ISO 178 | |
120 °C | 90 MPa Show Supplier Material materials with Flexural yield strength of 90 MPa | dry | ISO 178 | |
160 °C | 55.0 MPa Show Supplier Material materials with Flexural yield strength of 55.0 MPa | dry | ISO 178 | |
200 °C | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | dry | ISO 178 | |
Módulo de flexión | 8 GPa Show Supplier Material materials with Módulo de flexión of 8 GPa | dry | ISO 178 | |
120 °C | 6.9 GPa Show Supplier Material materials with Módulo de flexión of 6.9 GPa | dry | ISO 178 | |
160 °C | 2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | dry | ISO 178 | |
200 °C | 2.1 GPa Show Supplier Material materials with Módulo de flexión of 2.1 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 |
9.5 GPa Show Supplier Material materials with Módulo elástico of 9.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 4.6 GPa Show Supplier Material materials with Módulo elástico of 4.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 2 GPa Show Supplier Material materials with Módulo elástico of 2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 175 MPa Show Supplier Material materials with Resistencia a la tracción of 175 MPa | dry | ISO 527-1/-2 |
145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | dry | ISO 527-1/-2 | ||
120 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
160 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | dry | ISO 527-1/-2 | |
200 °C | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 18.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 18.5 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU | |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 180/1U |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.4e-07 1/K | dry | ISO 11359-1/-2 | parallel, above Tg | |
1.8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | normal, above Tg | ||
Inflamabilidad | HB | dry | IEC 60695-11-10 | UL recognition :Yes | |
Temperatura de flexión bajo carga | 250 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 250 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 90 °C Show Supplier Material materials with Temperatura de transición del vidrio of 90 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 60250 | 1GHz |
3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 60250 | 5GHz | |
Factor de disipación | 30 [-] Show Supplier Material materials with Factor de disipación of 30 [-] | dry | IEC 60250 | 1GHz |
50 [-] Show Supplier Material materials with Factor de disipación of 50 [-] | dry | IEC 60250 | 5GHz | |
Rigidez dieléctrica | 36 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 36 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 175 V Show Supplier Material materials with Índice de seguimiento comparativo of 175 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Pipe Fittings, Endlaminates (electro motors), Automotive e-motor Bobbins | |
Certifications | Food Contact, Drinking Water | |
Fillers | 30% Glass Fiber |