General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 225 MPa Show Supplier Material materials with Flexural yield strength of 225 MPa | dry | ISO 178 | |
Módulo de flexión | 8.7 GPa Show Supplier Material materials with Módulo de flexión of 8.7 GPa | dry | ISO 178 | |
Módulo elástico | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Ball pressure temperature | 255 °C Show Supplier Material materials with Ball pressure temperature of 255 °C | dry | IEC 60695-10-2 | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | |
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | ||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 60 °C Show Supplier Material materials with Temperatura de transición del vidrio of 60 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Rigidez dieléctrica | 40 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 40 kV/mm | dry | IEC 60243-1 | |
Índice de seguimiento comparativo | - | dry | Sim. to IEC 60112 | Above 600V |
600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | EV Charging Plugs | |
Certifications | Yellow Card Available | |
Fillers | 25% Glass Fiber |