General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4 % Show Supplier Material materials with Absorción de agua of 4 % | dry | Sim. to ISO 62 |
Densidad | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.3 % Show Supplier Material materials with Elongación of 3.3 % | dry | ISO 527-1/-2 | |
3.5 % Show Supplier Material materials with Elongación of 3.5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 15 % Show Supplier Material materials with Elongación of 15 % | dry | ISO 527-1/-2 | |
140 °C | 14.0 % Show Supplier Material materials with Elongación of 14.0 % | dry | ISO 527-1/-2 | |
160 °C | 13 % Show Supplier Material materials with Elongación of 13 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 255 MPa Show Supplier Material materials with Flexural yield strength of 255 MPa | conditioned | ISO 178 | |
285 MPa Show Supplier Material materials with Flexural yield strength of 285 MPa | dry | ISO 178 | ||
Módulo de flexión | 9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | conditioned | ISO 178 | |
9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | dry | ISO 178 | ||
Módulo elástico | 9.3 GPa Show Supplier Material materials with Módulo elástico of 9.3 GPa | conditioned | ISO 527-1/-2 | |
9.5 GPa Show Supplier Material materials with Módulo elástico of 9.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | dry | ISO 527-1/-2 | |
140 °C | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | conditioned | ISO 527-1/-2 | |
190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | dry | ISO 527-1/-2 | ||
120 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |
140 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |
160 °C | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.5 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 8.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7.5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Inflamabilidad | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
230 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 230 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Drinking Water, Yellow Card Available | |
Fillers | 30% Glass Fiber |