General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 |
2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | ||
120 °C | 6.8 % Show Supplier Material materials with Elongación of 6.8 % | dry | ISO 527-1/-2 | |
160 °C | 8.5 % Show Supplier Material materials with Elongación of 8.5 % | dry | ISO 527-1/-2 | |
200 °C | 9 % Show Supplier Material materials with Elongación of 9 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 205 MPa Show Supplier Material materials with Flexural yield strength of 205 MPa | dry | ISO 178 | |
120 °C | 88 MPa Show Supplier Material materials with Flexural yield strength of 88 MPa | dry | ISO 178 | |
160 °C | 55.0 MPa Show Supplier Material materials with Flexural yield strength of 55.0 MPa | dry | ISO 178 | |
200 °C | 38 MPa Show Supplier Material materials with Flexural yield strength of 38 MPa | dry | ISO 178 | |
Módulo de flexión | 7.9 GPa Show Supplier Material materials with Módulo de flexión of 7.9 GPa | dry | ISO 178 | |
120 °C | 6.8 GPa Show Supplier Material materials with Módulo de flexión of 6.8 GPa | dry | ISO 178 | |
160 °C | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | dry | ISO 178 | |
200 °C | 2 GPa Show Supplier Material materials with Módulo de flexión of 2 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 9.8 GPa Show Supplier Material materials with Módulo elástico of 9.8 GPa | dry | ISO 527-1/-2 |
9.3 GPa Show Supplier Material materials with Módulo elástico of 9.3 GPa | dry | ISO 527-1/-2 | ||
120 °C | 4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-1/-2 | |
200 °C | 1.9 GPa Show Supplier Material materials with Módulo elástico of 1.9 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 165 MPa Show Supplier Material materials with Resistencia a la tracción of 165 MPa | dry | ISO 527-1/-2 |
140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | dry | ISO 527-1/-2 | ||
120 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | dry | ISO 527-1/-2 | |
160 °C | 48 MPa Show Supplier Material materials with Resistencia a la tracción of 48 MPa | dry | ISO 527-1/-2 | |
200 °C | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU | |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 180/1U |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.4e-07 1/K | dry | ISO 11359-1/-2 | parallel, above Tg | |
1.8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | normal, above Tg | ||
Temperatura de flexión bajo carga | 250 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 250 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 280 °C Show Supplier Material materials with Temperatura de fusión of 280 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 90 °C Show Supplier Material materials with Temperatura de transición del vidrio of 90 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 36 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 36 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Índice de seguimiento comparativo | 175 V Show Supplier Material materials with Índice de seguimiento comparativo of 175 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | ADAS Radar Housing | |
Fillers | 30% Glass Fiber |