General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.25 % Show Supplier Material materials with Absorción de agua of 0.25 % | dry | Sim. to ISO 62 |
Densidad | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |
Módulo elástico | 11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 155 MPa Show Supplier Material materials with Resistencia a la tracción of 155 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | dry | ISO 179/1eA |
23 °C | 9.7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9.7 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 9.01e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 9.01e-08 mm²/s | dry | - | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 213 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 213 °C | dry | ISO 75-1/-2 | 2 MPa | ||
224 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 224 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Índice de seguimiento comparativo | 475 V Show Supplier Material materials with Índice de seguimiento comparativo of 475 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | Sim. to ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1260 g/cm³ Show Supplier Material materials with Density of melt of 1260 g/cm³ | dry | - | |
Specific heat capacity melt | 1740.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1740.0 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.197 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.197 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Yellow Card Available | |
Fillers | 35% Glass Fiber |