General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.65 % Show Supplier Material materials with Absorción de agua of 2.65 % | dry | ISO 62 | at 23°C after 24h |
9.5 % Show Supplier Material materials with Absorción de agua of 9.5 % | dry | Sim. to ISO 62 | ||
Densidad | 1.41 g/cm³ Show Supplier Material materials with Densidad of 1.41 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.6 % Show Supplier Material materials with Moisture absorption of 2.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-1/-2 | |
14.0 % Show Supplier Material materials with Elongación of 14.0 % | conditioned | ISO 527-1/-2 | ||
120 °C | 30 % Show Supplier Material materials with Elongación of 30 % | dry | ISO 527-1/-2 | |
160 °C | 29.0 % Show Supplier Material materials with Elongación of 29.0 % | dry | ISO 527-1/-2 | |
180 °C | 28.0 % Show Supplier Material materials with Elongación of 28.0 % | dry | ISO 527-1/-2 | |
200 °C | 27 % Show Supplier Material materials with Elongación of 27 % | dry | ISO 527-1/-2 | |
Módulo elástico | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | conditioned | ISO 527-1/-2 | |
4.7 GPa Show Supplier Material materials with Módulo elástico of 4.7 GPa | dry | ISO 527-1/-2 | ||
120 °C | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.9 GPa Show Supplier Material materials with Módulo elástico of 0.9 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.8 GPa Show Supplier Material materials with Módulo elástico of 0.8 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.74 GPa Show Supplier Material materials with Módulo elástico of 0.74 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | conditioned | ISO 527-1/-2 | |
90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 | ||
120 °C | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | |
160 °C | 35 MPa Show Supplier Material materials with Resistencia a la tracción of 35 MPa | dry | ISO 527-1/-2 | |
180 °C | 32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | dry | ISO 527-1/-2 | |
200 °C | 30 MPa Show Supplier Material materials with Resistencia a la tracción of 30 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 235 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 235 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 60250 | 1GHz |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.4 [-] Show Supplier Material materials with Constante dieléctrica of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.6 [-] Show Supplier Material materials with Constante dieléctrica of 4.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
12 [-] Show Supplier Material materials with Constante dieléctrica of 12 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 80 [-] Show Supplier Material materials with Factor de disipación of 80 [-] | dry | IEC 62631-2-1 | 100Hz |
230 [-] Show Supplier Material materials with Factor de disipación of 230 [-] | dry | IEC 62631-2-1 | 1MHz | |
300 [-] Show Supplier Material materials with Factor de disipación of 300 [-] | dry | IEC 60250 | 1GHz | |
900 [-] Show Supplier Material materials with Factor de disipación of 900 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1500 [-] Show Supplier Material materials with Factor de disipación of 1500 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+09 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+09 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | Sim. to ISO 294-4 | Parallel |
1.7 % Show Supplier Material materials with Contracción of 1.7 % | dry | Sim. to ISO 294-4 | Normal | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Bead |