Material: el 'Polyamide Nylon 6' que buscabas ha sido remplazado por el material siguiente.

Akulon® K224-G6

Nombres alternativos y comerciales
PA6-GF30
Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® K224-G6

Los datos sobre este material han sido proporcionados por DSM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueConditionTesting Standard

Absorción de agua

6.3 %

Show Supplier Material materials with Absorción de agua of 6.3 %

dry

Sim. to ISO 62

Densidad

1.35 g/cm³

Show Supplier Material materials with Densidad of 1.35 g/cm³

dry

ISO 1183

Moisture absorption

1.9 %

Show Supplier Material materials with Moisture absorption of 1.9 %

dry

Sim. to ISO 62

Mecánica

PropertyTemperatureValueConditionTesting StandardComment

Dureza Shore D

85 [-]

Show Supplier Material materials with Dureza Shore D of 85 [-]

dry

ISO 868

15s

Elongación

-40 °C

3 %

Show Supplier Material materials with Elongación of 3 %

dry

ISO 527-1/-2

3.8 %

Show Supplier Material materials with Elongación of 3.8 %

dry

ISO 527-1/-2

7 %

Show Supplier Material materials with Elongación of 7 %

conditioned

ISO 527-1/-2

Flexural yield strength

165 MPa

Show Supplier Material materials with Flexural yield strength of 165 MPa

conditioned

ISO 178

290 MPa

Show Supplier Material materials with Flexural yield strength of 290 MPa

dry

ISO 178

Módulo de flexión

5.3 GPa

Show Supplier Material materials with Módulo de flexión of 5.3 GPa

conditioned

ISO 178

9.2 GPa

Show Supplier Material materials with Módulo de flexión of 9.2 GPa

dry

ISO 178

Módulo elástico

-40 °C

10.4 GPa

Show Supplier Material materials with Módulo elástico of 10.4 GPa

dry

ISO 527-1/-2

6 GPa

Show Supplier Material materials with Módulo elástico of 6 GPa

conditioned

ISO 527-1/-2

9.7 GPa

Show Supplier Material materials with Módulo elástico of 9.7 GPa

dry

ISO 527-1/-2

100 °C

4.3 GPa

Show Supplier Material materials with Módulo elástico of 4.3 GPa

dry

ISO 527-1/-2

Resistencia a la tracción

-40 °C

235 MPa

Show Supplier Material materials with Resistencia a la tracción of 235 MPa

dry

ISO 527-1/-2

110 MPa

Show Supplier Material materials with Resistencia a la tracción of 110 MPa

conditioned

ISO 527-1/-2

185 MPa

Show Supplier Material materials with Resistencia a la tracción of 185 MPa

dry

ISO 527-1/-2

100 °C

95 MPa

Show Supplier Material materials with Resistencia a la tracción of 95 MPa

dry

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-30 °C

11 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m²

dry, conditioned

ISO 179/1eA

23 °C

14.0 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m²

dry

ISO 179/1eA

23 °C

25 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m²

conditioned

ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

-30 °C

75 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m²

dry, conditioned

ISO 179/1eU

23 °C

95 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 95 kJ/m²

dry

ISO 179/1eU

23 °C

110 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 110 kJ/m²

conditioned

ISO 179/1eU

Aplicaciones térmicas

PropertyValueConditionTesting StandardThicknessPressureComment

Ball pressure temperature

215 °C

Show Supplier Material materials with Ball pressure temperature of 215 °C

dry

IEC 60695-10-2

Coeficiente de dilatación térmica

2e-07 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K

dry

ISO 11359-1/-2

Parallel

7e-07 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K

dry

ISO 11359-1/-2

Normal

Difusividad térmica

1.12e-07 mm²/s

Show Supplier Material materials with Difusividad térmica of 1.12e-07 mm²/s

dry

-

Inflamabilidad

HB

dry

IEC 60695-11-10

1.5 mm

UL recognition :Yes

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

dry

UL746B

0.75 mm

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

dry

UL746B

0.75 mm

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

dry

UL746B

0.75 mm

Temperatura de flexión bajo carga

207 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 207 °C

dry

ISO 75-1/-2

2 MPa

220 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C

dry

ISO 75-1/-2

0.45 MPa

Temperatura de fusión

220 °C

Show Supplier Material materials with Temperatura de fusión of 220 °C

dry

ISO 11357-1/-3

10°C/min

Temperatura de reblandecimiento Vicat

216 °C

Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 216 °C

dry

ISO 306

50°C/h 50N

Eléctrico

PropertyValueConditionTesting StandardComment

Constante dieléctrica

3.3 [-]

Show Supplier Material materials with Constante dieléctrica of 3.3 [-]

dry

IEC 62631-2-1

1MHz

3.5 [-]

Show Supplier Material materials with Constante dieléctrica of 3.5 [-]

dry

IEC 62631-2-1

100Hz

5 [-]

Show Supplier Material materials with Constante dieléctrica of 5 [-]

conditioned

IEC 62631-2-1

1MHz

20 [-]

Show Supplier Material materials with Constante dieléctrica of 20 [-]

conditioned

IEC 62631-2-1

100Hz

Factor de disipación

50 [-]

Show Supplier Material materials with Factor de disipación of 50 [-]

dry

IEC 62631-2-1

100Hz

150 [-]

Show Supplier Material materials with Factor de disipación of 150 [-]

dry

IEC 62631-2-1

1MHz

1200 [-]

Show Supplier Material materials with Factor de disipación of 1200 [-]

conditioned

IEC 62631-2-1

1MHz

3000 [-]

Show Supplier Material materials with Factor de disipación of 3000 [-]

conditioned

IEC 62631-2-1

100Hz

Rigidez dieléctrica

25 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm

conditioned

IEC 60243-1

30 kV/mm

Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm

dry

IEC 60243-1

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

conditioned

IEC 62631-3-2

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

conditioned

IEC 62631-3-1

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

dry

IEC 62631-3-1

Índice de seguimiento comparativo

600 V

Show Supplier Material materials with Índice de seguimiento comparativo of 600 V

conditioned

IEC 60112

Rheological Properties

PropertyTemperatureValueConditionTesting StandardComment

Contracción

0.3 %

Show Supplier Material materials with Contracción of 0.3 %

dry

ISO 294-4

Parallel

0.9 %

Show Supplier Material materials with Contracción of 0.9 %

dry

ISO 294-4

Normal

Density of melt

1150 g/cm³

Show Supplier Material materials with Density of melt of 1150 g/cm³

dry

-

Specific heat capacity melt

2110 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2110 J/(kg·K)

dry

-

Thermal conductivity of melt

0.27 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K)

dry

-

Velocidad de flujo de la masa derretida

240 °C

7.3 g/10min

Show Supplier Material materials with Velocidad de flujo de la masa derretida of 7.3 g/10min

dry

ISO 1133

Velocidad de flujo del volumen derretido

240 °C

6.4 cm³/10min

Show Supplier Material materials with Velocidad de flujo del volumen derretido of 6.4 cm³/10min

dry

ISO 1133

Technological properties

Property
Application areas

Chainsaw housings, Chair Bases, Chair Arms, Chair Frames, Powertool Housings, Wheel Chair Rims, Railway Insulation Plates, Rear Grips, Wheels, Structural Reinforcements

Certifications

Yellow Card Available

Fillers

30% Glass Fiber