General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.62 g/cm³ Show Supplier Material materials with Densidad of 1.62 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 84 [-] Show Supplier Material materials with Dureza Shore D of 84 [-] | ASTM D785 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 80 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 14.5 GPa Show Supplier Material materials with Módulo de flexión of 14.5 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 200 MPa Show Supplier Material materials with Resistencia a la flexión of 200 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la tracción of 179 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de flexión bajo carga | 279 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 279 °C | ASTM D648 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.8 [-] Show Supplier Material materials with Constante dieléctrica of 3.8 [-] | ASTM D147 |
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+16 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+16 Ω/sq | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive bumpers, Automotive applications, Automotive exterior parts | |
Fillers | 40% Glass Fiber |