General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Densidad of 1.56 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.6 % Show Supplier Material materials with Elongación of 1.6 % | ASTM D638 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 78 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 78 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 12 GPa Show Supplier Material materials with Módulo de flexión of 12 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 180 MPa Show Supplier Material materials with Resistencia a la flexión of 180 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | ASTM D638 |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | ASTM D147 |
Surface resistivity | 23.0 °C | 1.00E+16 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+16 Ω/sq |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | ASTM D955(GB15585), Molding Shrinkage |
Technological properties
Property | ||
---|---|---|
Application areas | Automobiles, electronic appliances and home appliances,Connector, switch, DVD laser head, coil frame, gearbox, circuit board, lamp holder, reflector lamp cup and bracket, throttle body, junction box, oil pump impeller, valve body, LED lamp housing, thermal circuit board, heat dissipation element etc | |
Fillers | 30% Glass Fiber |